Re: [MW:16029] Class-II used instead of Class I film

Convince can made by deviation request.
 
otherwise redo. refer the attchd sht.
 
 
 
Regards,
S.SENTHILKUMAR
From: Nandesh Kumar <nandeshkumar@rocketmail.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, 21 November 2012 9:23 PM
Subject: Re: [MW:15997] Class-II used instead of Class I film

Using class - II film instaed of class - I film need not be a reason for rejection, provided, if you have achieved the required density and sensitivity. Convince your client and do not repeat it in future.

ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,
Nandesh Kumar A

Abu Dhabi, UAE

P.S. : Please don't print this e-mail unless you really need to.


--- On Wed, 21/11/12, mohd <mohd52100@gmail.com> wrote:

From: mohd <mohd52100@gmail.com>
Subject: [MW:15984] Class-II used instead of Class I film
To: materials-welding@googlegroups.com
Date: Wednesday, 21 November, 2012, 9:01 AM

Dear all,
Our RT subcontractor used by mistakes Class-II (kodak)film instead of class-I (Kodak)
Pipe Materials : 8" API 5L GrB  thk : 8.18mm. No of Joints : 35 Joints.
As per Spec : Class-I required for thickness less than 12.7mm.
Client rejects all RT films.
Any possible solution?
regards,
mohd.
-- To post to this group, send email to materials-welding@googlegroups.comTo unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.comFor more options, visit this group's bolg at http://materials-welding.blogspot.com/http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.  
-- To post to this group, send email to materials-welding@googlegroups.comTo unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.comFor more options, visit this group's bolg at http://materials-welding.blogspot.com/http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.  

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...