Wednesday, November 21, 2012

Re: [MW:16003] Class-II used instead of Class I film

I to agree with Mr.Nandesh mail,in addition to that you may take a % Check shot by using Class-I films and convince your client.
Sent on my BlackBerry® from Vodafone

From: Nandesh Kumar <nandeshkumar@rocketmail.com>
Sender: materials-welding@googlegroups.com
Date: Wed, 21 Nov 2012 23:53:43 +0800 (SGT)
To: <materials-welding@googlegroups.com>
ReplyTo: materials-welding@googlegroups.com
Subject: Re: [MW:15997] Class-II used instead of Class I film


Using class - II film instaed of class - I film need not be a reason for rejection, provided, if you have achieved the required density and sensitivity. Convince your client and do not repeat it in future.

ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,

Nandesh Kumar A

Abu Dhabi, UAE

P.S. : Please don't print this e-mail unless you really need to.


--- On Wed, 21/11/12, mohd <mohd52100@gmail.com> wrote:

From: mohd <mohd52100@gmail.com>
Subject: [MW:15984] Class-II used instead of Class I film
To: materials-welding@googlegroups.com
Date: Wednesday, 21 November, 2012, 9:01 AM

Dear all,

Our RT subcontractor used by mistakes Class-II (kodak)film instead of class-I (Kodak)

Pipe Materials : 8" API 5L GrB  thk : 8.18mm. No of Joints : 35 Joints.

As per Spec : Class-I required for thickness less than 12.7mm.

Client rejects all RT films.

Any possible solution?

regards,
mohd.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...