[MW:15827] PQR with Filler wire ER316L Flux SA Cs2 Cr DC can e used on SS304L base metal

Dear Experts 

 PQR with Filler wire ER316L Flux SA Cs2 Cr DC; base metal base SA 240 SS316L.

Can we use this PQR to weld base metal SA 240 SS304/304L without changing Flux with 308L filler wire! Or re-qualification is required.

 

Thanks & regards

Ali Mhaskar,

UAE 

 

 

 

                   

 

 

Note: To protect against computer viruses, e-mail programs may prevent sending or receiving certain types of file attachments.  Check your e-mail security settings to determine how attachments are handled.

 

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...