Thursday, July 19, 2012

[MW:14897] 45 deg. elbow

Yes possible, you can make two 45 deg. elbows out of a 90 deg.elbow provided it meets your dimensional requirements.

sridhar.

From: eng ahmed <eng_ahmed450@yahoo.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Cc: c sridhar <sridhar305@yahoo.com>; Joy Pal <joypal79@gmail.com>; Lakine <lakine85@gmail.com>; Lakine <lakine85@gmail.com>; Saravanan Sornam <saravanshyla@gmail.com>
Sent: Thursday, 19 July 2012 11:32 AM
Subject: dear experts

Dear experts,
Can i make two 45 degree elbows by cut from 90 degree elbow?
The material is A234 Gr Wpb.
Best Regards
 
       

       Eng: Ahmed Gomaa
         QA/QC Engineer
                EGYPT
Email: Eng_ahmed450@yahoo.com
 Cell:   00201111350805


No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...