[SUSPECTED SPAM] Re: [MW:14681] P1 Material Pipe welding Joints RT and MT before PWHT is Acceptable or not ?


----- Original Message -----
From: mpk mpk
To: materials-welding
Sent: Mon, 25 Jun 2012 15:18:08 +0530 (IST)
Subject: [MW:14676] P1 Material Pipe welding Joints RT and MT before PWHT is Acceptable or not ?


Dear friend,

It can be acceptable but, only for internal judgement of workmanship/quality of weld (i.e.to observed any repair etc.) but If your job requirement is heat treatment you must go for RT after Heat treatment eventhough you attend RT or any NDT (as required)  before heat treatment & it may be acceptable before heattreatment .

Regards,
RKVichare






Dear experts,


P1
Material Pipe welding Joints  RT
and MT examination  before PWHT  is Acceptable or not ?



As per 2010  ASME B.31.3 para 341.3 Examination requirements,


(a) for P.nos 3,4 and 5 materials Examination shall be performed after completion of any heat treatment.


Thank you


YEM.





--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...