1. weld access hole must required prior to start welding as per fig 5.29.
 
2. CJP WPS can be used for PJP no need special WPS for PJP as per AWS D1.1
 
BHUVANESH

On 27 June 2012 10:09, cnooc <fzhang007@gmail.com> wrote:
I have several confusions on the use of AWS D1.1,can anyone help me ?

  • Is weld access holes/beam copes on web mandatory ? or as long as the welder can meet the penetration requirement,the fabricator can do the welding without the weld access hole?
  • Can i use a CJP WPS(use the same process,parameter...) to weld a PJP weld or filler weld without made a new WPS for PJP welds or filler welds?
Thanks !

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...