Re: [MW:14713] Re: welding procedure qualification requirement for P No.1 Group no 1,2

Can , The lower the temperature the more its brittle
 
Regards,
Kavin Murugam
0126159644
 

From: SUBHANKAR CHAKRABORTY <subh.tinny@gmail.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, June 27, 2012 12:15 PM
Subject: [MW:14701] Re: welding procedure qualification requirement for P No.1 Group no 1,2

Dear Exparts,
CAN ANYBODY EXPLAIN ME IF A PQR P1G2 ~ P1G2 QUALIFIED WITH IMPACT AT -48 DEGREE,IS IT SUPPORT A WPS P1G2 ~ P1G2 WITH IMPACT AT -29?
 
SUBHANKAR CHAKRABORTY

On Thursday, 21 June 2012 14:17:17 UTC+5:30, LALIT wrote:
Dear expert,
 
If welding procedure is qualified for the SA 516 Gr.60 to same (P No.1 Group 1 to same), then is it required to conduct another PQR for the SA 516 Gr.70 to same (P No.1 Group 2 to same), if impact requirement is applicable for both material at same temperature?


--
Regards

Lalit Vadadoriya
Sr.Engineer (Inspection)
Engineers India Limited

Dahej Petrochemical Complex,
Dahej (Gujarat)

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...