Dear Venkat,
 
Kindly refer SA20 ASME Sec II Part A.
MT=Heat treated
LTV=CVN done.
ZT= no idea
 
Kavin Murugam
0126159644
 

From: "g.venkatesan06@gmail.com" <g.venkatesan06@gmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Thursday, June 28, 2012 2:29 AM
Subject: [MW:14709] Explanation of MTLTV ZT-Reg

Dear sir.
I saw one carbon steel MTC SA 537 CL 1 MTLTV ZT.

What is the explanation of MTLTV ZT.

Which source or code gives that explanation.
Kindly guide me.

Regards
venkat
trichy

----------
Sent from my Nokia phone

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...