Wednesday, June 27, 2012

Re: [MW:14708] GTAW wires equivalent to AWS E10018-D2 and E 11018M

  as per AWS 5.28   ER 110S-G
 
Chandrakant Sarvade
09769554718

--- On Wed, 27/6/12, ARC WELDING COMPANY <arcweldingcom@gmail.com> wrote:

From: ARC WELDING COMPANY <arcweldingcom@gmail.com>
Subject: [MW:14702] GTAW wires equivalent to AWS E10018-D2 and E 11018M
To: materials-welding@googlegroups.com
Cc: arcweldingcompany@gmail.com
Date: Wednesday, 27 June, 2012, 5:26 AM

Dear sir,

Can anybody suggest GTAW consumables equivalent to AWS E10018-D2 and E 11018M?

Thanks and regards,

For Arc Welding Company,

Anil Verma

9999200148

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...