Re: [MW:14707] suitable electrodes for 40 CR to IS 2062 Gr B

40Cr, is a kind of HSLA.
 
 
the suitble electrode for 40Cr is :
1, SMAW: Phoenix SH Ni 2 K 130
2, GMAW: Union X 90
 
Please log on http://www.t-put.com/ for more details.
 
Roy
Bohler Welding Group
 
 
From: suresh
Sent: Wednesday, June 27, 2012 5:45 PM
Subject: [MW:14706] suitable electrodes for 40 CR to IS 2062 Gr B
 
Dear All,
i would like to know physical properties and chemical compositions of 40 CR material.
what is the suitable electrode for 40 CR to IS 2062 G
Thanks and Regards,
Suresh.
 
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...