Dear Mohd,

The Advantages are:

01.Can avoid tacking on the parent metal outside the joint which will save damages to base metal, reduces the rework required.
02.Accurate alignment.

But there may be some restrictions also there with the clamps .i.e it may not be capable to  use in the lengthy jobs / Heavy wall pipes .

With Best regards

Phani kumar

On Mon, Jun 18, 2012 at 11:34 AM, manpreet <manpreetsin88@rediffmail.com> wrote:


On Mon, 18 Jun 2012 11:24:53 +0530 wrote
>Dear experts

Hi,

External Clamps are allowed only for Tie-In joints or for short pipelines ans small diameter (<6 in.)

At least 50% of root pass is to be completed before the external clamp is released,
Internal alignment clamps are preferred for better alignment and not released until 100% of the root pass is complete.

Misalignment between the internal surfaces shall not exceed the lesser of 3mm or 1% of the pipe internal diameter at any point, more restrictions are set for Pipelines subject to strain.


Regards,
Manpreet Singh

what are advatages and disadvantages of using external clamps&

Internal clamps in Pipeline.



We'r doing 30"pipe line projects and client insist us to use only

Internal clamps for fitup pupose.



regards,

mohd



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...