There is no specific temperature and limit for humidity, for storage, manufacturer's recommendation is to store at dry place and at room temperature, Most of consumable are supplied in sealed packs or plastic bags so they will not absorb moisture until there is damage with packing, once you open these bags for use then further caution and manufactures instruction should be followed about drying and baking or reuse.

Regards,


On Mon, Jun 25, 2012 at 9:17 AM, Himan Nikdin <himannikdin@gmail.com> wrote:
Dear Mr. Tariq

1-you can follow ASME SEC II-part C specifications which describes the storing and handling conditions for MMA, SAW flux and wires.meanwhile manufacturers recommendations will be helpful.
 
2-If you could not maintain storing conditions it causes many defects during and after welding.

Regards,
Himan

On Sun, Jun 24, 2012 at 9:01 PM, Tariq Hussain <tariqhussain632@gmail.com> wrote:
Dear Experts,

Kindly Provide Your Valuable View on Below Queries.

1. What is Recommended Procedure / Conditions for storage of MMA electrodes, SAW Wire Spools, TIG Wires & SAW Fluxes in term of Consumable Storage Room Temperature Relative  Humidity?


2. What to do if we could not maintain the Required Consumable Storage Room Temperature and Relative Humidity


Thanks & Regards


Tariq Hussain 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...