Monday, June 25, 2012

Re: [MW:14674] Storage Conditions of Welding Consumables.

Dear Mr. Tariq

1-you can follow ASME SEC II-part C specifications which describes the storing and handling conditions for MMA, SAW flux and wires.meanwhile manufacturers recommendations will be helpful.
 
2-If you could not maintain storing conditions it causes many defects during and after welding.

Regards,
Himan

On Sun, Jun 24, 2012 at 9:01 PM, Tariq Hussain <tariqhussain632@gmail.com> wrote:
Dear Experts,

Kindly Provide Your Valuable View on Below Queries.

1. What is Recommended Procedure / Conditions for storage of MMA electrodes, SAW Wire Spools, TIG Wires & SAW Fluxes in term of Consumable Storage Room Temperature Relative  Humidity?


2. What to do if we could not maintain the Required Consumable Storage Room Temperature and Relative Humidity


Thanks & Regards


Tariq Hussain 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...