As per QW-403;
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
"If, however, two or more qualification records have the same essential and supplementary essential variables, except that the base metals are assigned to different Group Numbers within the same P-Number, then the combination of base metals is also qualified. In addition, when base metals of two different P-Number Group Number combinations are qualified using a single test coupon, that coupon qualifies the welding of those two P-Number Group Numbers to themselves as well as to each other using the variables qualified."
So the answer of Q1 is "No" and Q2 is "Yes".
Regards
Himan
On Sat, Jun 23, 2012 at 5:07 AM, Kavin202082 <kavin202082@yahoo.com> wrote:
Nope , u need to qualify P1 G1 to P1 G2 supplementry essential. Once u qualify tis It wil cover P1 G1 TO P1 G1, P1G2 TO P1 G2 AND P1G1 TO P1G2.Combination of g1 &g2 in one pqr req, nt combination of both pqr
Sent from Samsung Mobile
-------- Original message --------
Subject: Re: [MW:14647] Impact WPS P1G1 to P1G1 &P1G2 to P1G2 Qualified P1G1 to P1G2 with impact ?
From: samshuddin k <sam.renja@gmail.com>
To: materials-welding@googlegroups.com
CC:1. No
2. Yes
On 6/22/12, mohd <mohd52100@gmail.com> wrote:
> Dear experts,
>
> Dear Expert,
>
> 1)Two PQR P1 G1 to P1 G1 & P1 G2 to P1 G2 with imapct, Qualified
>
> WPS With Impact P1G1 to P1G2 Ans : Yes Or NO.
>
> 2) PQR P1G1 to P1G2 with Impact,Qualified Following WPS,
>
> a) P1G1 to P1G1 with Imapact Ans Yes Or NO
> b) P1G2 to P1G2 with Impact Ans Yes or No.
>
> I thinks these answer more clarified Mr lalit Querry.
>
> Thanks,
> Mohd.
>
>
> On Jun 21, 9:47 am, LALIT VADADORIYA <lalit.vadador...@gmail.com>
> wrote:
>> Dear expert,
>>
>> If welding procedure is qualified for the SA 516 Gr.60 to same (P No.1
>> Group 1 to same), then is it required to conduct another PQR for the SA
>> 516
>> Gr.70 to same (P No.1 Group 2 to same), if impact requirement is
>> applicable
>> for both material at same temperature?
>>
>> --
>> Regards
>>
>> *Lalit Vadadoriya
>> Sr.Engineer (Inspection)
>> Engineers India Limited*
>> *Dahej Petrochemical Complex,*
>> *Dahej (Gujarat)*
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments