Re: [MW:14657] LWN flange...............

the contractor needs to resubmit their drawing and calcs for approval before you accept the proposed procedure. As you may know, the neck of a CL150 and CL300 LWN has a difference of about 1/8".

 
On Fri, Jun 22, 2012 at 6:33 AM, shanmugam govindarajan <rajansgr@yahoo.com> wrote:
 Dear Experts,

Please clarify the below problem.
Contractor has welded 2" 150# LWN flange with the vessel. Approved drawing requires 2" 300# LWN flange. Contractor proposes to cut and remove the bolting part of the LWN flange and weld with the 300# bolting part of LWN flange. Their intention is not to disturb the vessel and due to tight schedule. But I told them that entire LWNF shall be removed from the vessel and shall be welded with 300# LWNF. Contractor says calculation for both 150# and 300# is same , so there is no problem.

Please clarify whether this is a correct approach.
  
 

With regards,

Govi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...