Hi!
Generally to avoid more PQR qualification ,, while qualifying PQR of P1 Gr1 and P1 Gr2 instead of qualifying TWO separate PQR
It is better to Qualify PQR onone  testcoupon having one of the plates of P1 Gr1 and other plate of P1 Gr2  and for Impact test, test Weld , HAZ of both side i.e. P1Gr2 , and P1 Gr1
With these testing the PQR is qualified for a)P1 Gr1 to itself b) P1 Gr 2 to it self Satisfying all essential and supplimentary esentials
 
Regards
 
Hegde P.B.
 
 

--- On Fri, 22/6/12, samshuddin k <sam.renja@gmail.com> wrote:

From: samshuddin k <sam.renja@gmail.com>
Subject: Re: [MW:14647] Impact WPS P1G1 to P1G1 &P1G2 to P1G2 Qualified P1G1 to P1G2 with impact ?
To: materials-welding@googlegroups.com
Date: Friday, 22 June, 2012, 4:44 PM

1. No
2. Yes

On 6/22/12, mohd <mohd52100@gmail.com> wrote:
> Dear experts,
>
> Dear Expert,
>
> 1)Two PQR P1 G1 to P1 G1 & P1 G2 to P1 G2 with imapct, Qualified
>
>  WPS With Impact P1G1 to P1G2 Ans : Yes Or NO.
>
> 2) PQR P1G1 to P1G2 with Impact,Qualified Following WPS,
>
>    a) P1G1 to P1G1 with Imapact  Ans Yes Or NO
>    b) P1G2 to P1G2 with Impact   Ans Yes or No.
>
> I thinks these answer more clarified Mr lalit Querry.
>
> Thanks,
> Mohd.
>
>
> On Jun 21, 9:47 am, LALIT VADADORIYA <lalit.vadador...@gmail.com>
> wrote:
>> Dear expert,
>>
>> If welding procedure is qualified for the SA 516 Gr.60 to same (P No.1
>> Group 1 to same), then is it required to conduct another PQR for the SA
>> 516
>> Gr.70 to same (P No.1 Group 2 to same), if impact requirement is
>> applicable
>> for both material at same temperature?
>>
>> --
>> Regards
>>
>> *Lalit Vadadoriya
>> Sr.Engineer (Inspection)
>> Engineers India Limited*
>> *Dahej Petrochemical Complex,*
>> *Dahej (Gujarat)*
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...