Re: [MW:14652] Impact WPS P1G1 to P1G1 &P1G2 to P1G2 Qualified P1G1 to P1G2 with impact ?



On Fri, Jun 22, 2012 at 2:10 PM, mohd <mohd52100@gmail.com> wrote:
Dear experts,

Dear Expert,

1)Two PQR P1 G1 to P1 G1 & P1 G2 to P1 G2 with imapct, Qualified

 WPS With Impact P1G1 to P1G2 Ans : Yes Or NO.
 
Ans: Yes

2) PQR P1G1 to P1G2 with Impact,Qualified Following WPS,

  a) P1G1 to P1G1 with Imapact  Ans Yes Or NO
 
Ans: Yes
 
  b) P1G2 to P1G2 with Impact   Ans Yes or No.
 
 
Ans: Yes

I thinks these answer more clarified Mr lalit Querry.

Thanks,
Mohd.


On Jun 21, 9:47 am, LALIT VADADORIYA <lalit.vadador...@gmail.com>
wrote:
> Dear expert,
>
> If welding procedure is qualified for the SA 516 Gr.60 to same (P No.1
> Group 1 to same), then is it required to conduct another PQR for the SA 516
> Gr.70 to same (P No.1 Group 2 to same), if impact requirement is applicable
> for both material at same temperature?
>
> --
> Regards
>
> *Lalit Vadadoriya
> Sr.Engineer (Inspection)
> Engineers India Limited*
> *Dahej Petrochemical Complex,*
> *Dahej (Gujarat)*

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...