Re: [MW:14631] Allowable temp range for SS316/316L

Dear Mr Bagesh,

I have worked with cryogenic field where MDTM is up to -196 Deg Celcius and flange used for the field of cryogenics we used that same material : ASTM A 182 Gr F 316L.In my opinion there will be  no problem to use this flanges for lower temperature services.

Regards

Yash
 


On Wed, Jun 20, 2012 at 5:35 PM, Bagesh Kumar <bagesh.kmr@gmail.com> wrote:

Dear friends...

Below is the query posted by my friend...

Regards..
Bagesh

On Jun 20, 2012 3:47 PM, "Narendra Singh" <ns.mech@gmail.com> wrote:

Good Morning Sir,

 

Hope things are fine at your end.

 

Sir I have one query on using flanged forged material  ASTM A182 Gr F316L (B16.5) for weld neck flange at temp (-)70 deg C., however B16.5 doesn't tabulated any equivalent pressure (Group-2.3 per B16.5)below -29 C. Is this material suitable for temperature -70 degree Centigrade while ASME B16.5 doesn't provide any allowable at this temperature.

 

Actually In one of my project PMS having temp range of -75 to 150 Deg C, and tabulated ASTM A182 Gr F316L (B16.5) for flanges. My piping has operating temperature of -70 Deg C and Design 85 Deg C.

I need to check flange leakage but unfortunately no allowable values given in B16.5.

 

I request your expert views on above.

 

 
--------------------------
Thanks & Regards
Narendra Singh
GSM: 9818696721
Mail:
ns.mech@gmail.com
 
$ Please dont print this email unless you really need to $

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...