[MW:14703] AWS D1.1 WPS qualification range?

I have several confusions on the use of AWS D1.1,can anyone help me ?

  • Is weld access holes/beam copes on web mandatory ? or as long as the welder can meet the penetration requirement,the fabricator can do the welding without the weld access hole?
  • Can i use a CJP WPS(use the same process,parameter...) to weld a PJP weld or filler weld without made a new WPS for PJP welds or filler welds?
Thanks !

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...