Dear experts,
Dear Expert,
1)Two PQR P1 G1 to P1 G1 & P1 G2 to P1 G2 with imapct, Qualified
WPS With Impact P1G1 to P1G2 Ans : Yes Or NO.
2) PQR P1G1 to P1G2 with Impact,Qualified Following WPS,
a) P1G1 to P1G1 with Imapact Ans Yes Or NO
b) P1G2 to P1G2 with Impact Ans Yes or No.
I thinks these answer more clarified Mr lalit Querry.
Thanks,
Mohd.
On Jun 21, 9:47 am, LALIT VADADORIYA <lalit.vadador...@gmail.com>
wrote:
> Dear expert,
>
> If welding procedure is qualified for the SA 516 Gr.60 to same (P No.1
> Group 1 to same), then is it required to conduct another PQR for the SA 516
> Gr.70 to same (P No.1 Group 2 to same), if impact requirement is applicable
> for both material at same temperature?
>
> --
> Regards
>
> *Lalit Vadadoriya
> Sr.Engineer (Inspection)
> Engineers India Limited*
> *Dahej Petrochemical Complex,*
> *Dahej (Gujarat)*
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Dear Expert,
1)Two PQR P1 G1 to P1 G1 & P1 G2 to P1 G2 with imapct, Qualified
WPS With Impact P1G1 to P1G2 Ans : Yes Or NO.
2) PQR P1G1 to P1G2 with Impact,Qualified Following WPS,
a) P1G1 to P1G1 with Imapact Ans Yes Or NO
b) P1G2 to P1G2 with Impact Ans Yes or No.
I thinks these answer more clarified Mr lalit Querry.
Thanks,
Mohd.
On Jun 21, 9:47 am, LALIT VADADORIYA <lalit.vadador...@gmail.com>
wrote:
> Dear expert,
>
> If welding procedure is qualified for the SA 516 Gr.60 to same (P No.1
> Group 1 to same), then is it required to conduct another PQR for the SA 516
> Gr.70 to same (P No.1 Group 2 to same), if impact requirement is applicable
> for both material at same temperature?
>
> --
> Regards
>
> *Lalit Vadadoriya
> Sr.Engineer (Inspection)
> Engineers India Limited*
> *Dahej Petrochemical Complex,*
> *Dahej (Gujarat)*
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments