Sunday, April 1, 2012

Re: [MW:14040] Welder Performance as per API 650, renewal of certificates.

 
 
(a) When he has not welded with a process during a
period of 6 months or more, his qualifications for that
process shall expire; unless, within the 6 month period,
prior to his expiration of qualification
 
See  this caluse on 322 if the welder is not welded for last 6 months then only a requalification calls for.
otherwise his RT records will be enough for renewal.
 
Unnikrishnan
Qatar

 
 

From: Biplab Pal <biplab.mech@googlemail.com>
To: materials-welding@googlegroups.com
Sent: Sunday, April 1, 2012 5:47 AM
Subject: [MW:14035] Welder Performance as per API 650, renewal of certificates.

Dear All,

I have qualified welders as per Sec IX, 2010. Construction code is API 650.
As Per API 650 clause 8.1.2.2 one spot radiograph shall be taken in
the first 3 m (10 ft) of completed vertical joint of each type and
thickness welded by each welder or welding operator.
As per Sec-IX, QW-322.2 Renewal of Qualification
(a) Renewal of qualification expired under
QW-322.1(a) may be made for any process by welding a
single test coupon of either plate or pipe, of any material,
thickness or diameter, in any position, and by testing of
that coupon as required by QW-301 and QW-302. A successful
test renews the welder or welding operator's previous
qualifications for that process for those materials,
thicknesses, diameters, positions, and other variables for
which he was previously qualified.
Providing the requirements of QW-304 and QW-305 are
satisfied, renewal of qualification under QW-322.1(a) may
be done on production work.
(b) Welders and welding operators whose qualifications
have been revoked under QW-322.1(b) above shall requalify.
Qualification shall utilize a test coupon appropriate to
the planned production work. The coupon shall be welded
and tested as required by QW-301 and QW-302. Successful
test restores the qualification.

I have a question that , What is the extent of examination and lowest
permissable repair for satisfactory performance of an welder.
Client code does not tell anything about that.
Please give me the answer.

--
Thanks & Regards
Biplab Pal
E-mail:   biplab.mech@gmail.com

Information in this email and any attachments is confidential and
intended solely for the use of the individual(s) to whom it is
addressed or otherwise directed. Please note that any views or
opinions presented in this email are solely those of the author and do
not necessarily represent those of the Company. Finally, the recipient
should check this email and any attachments for the presence of
viruses. Myself accepts no liability for any damage caused by any
virus transmitted by this email.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...