Tuesday, March 6, 2012

Re: [MW:13836] Metallographic test

Technology has been well advanced. Long ago I have come across insitu-metallography which is being done to determine the residual life of components and metallography study related to it. It is considered as non-destructive test.
 
I am not sure whether Welding and fabrication codes included these tests. The conventional macro and metallography tests performed inaccordance to Code is considered Destructive tests.
 
Thanks & Regards

J.Gerald Jayakumar
0091-9344954677
From: peyman hafezi <peymanhafezi@gmail.com>
To: materials-welding@googlegroups.com
Sent: Tuesday, March 6, 2012 12:41 PM
Subject: Re: [MW:13835] Metallographic test

Dear Friend
Actually metallography is a destructive test. How can anyone do metallography on main job or welding? For metallography you have to make a sample of welding or metal by cutting it and bring the sample to lab.
Besides, in this test the surface of sample is being etched by a weak acid! So something like corrosion occurs on the surface!
As a metallurgist I'm going to say that Metallography is a Destructive test.
Regards

On Tue, Mar 6, 2012 at 9:29 AM, I.K.Inspection Services <ikinspection@gmail.com> wrote:
Dear experts,
 
           I knew the Macro and metallographic examinations are destructive tests and even it is given in the TWI books but a friend of mine who tells these are NDT. Could someone clarify about this? Is both macro and metallography same?
 
regards
IK
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...