Hi,
For localized PWHT  the procedure given in AWS D 10.10. This might be used if API 6A/16A permits.
 
Manivannan.


On Fri, Mar 2, 2012 at 11:58 AM, Eswaran samikannu <eswaranaws@yahoo.co.in> wrote:
Good day to all,
 
We are one of the authorised repairing & Manufacturer  of OEM Cameron, VG & Shaffer BOP and riser pipes , I want to know thermocouples location / No of thermocouples vs Pipe size according to API 6A /API 16A for localaised stress relief (PWHT), Any one have the standards let me know or inform where i can get the information.
 
Thanks
S.Eswaran 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
MANIVANNAN.P

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...