Hi,
As per API 6A, it was clearly specified PWHT shall be as per WPS only,
PWHT shall be carried as per the written procedure(which shall specify the tolerance in the temperature also) by the manufacturer and complying to the WPS.
Further WPS shall be in accordance with ASME Sec IX.
So as per my view we can refer for ASME Sec VIII Div -1 UW 40,( For requirements) and UCS 56, UNF 56, UHT 56, UHA 56, (for the temperature range, thickness limits, soaking time, etc)
I hope we can follow ASME Sec VIII.
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Eswaran samikannu
Sent: Friday, March 02, 2012 11:59 AM
To: materials-welding@googlegroups.com
Subject: [MW:13803] Post Weld heat treatment & No of thermocouples regarding
Good day to all,
We are one of the authorised repairing & Manufacturer of OEM Cameron, VG & Shaffer BOP and riser pipes , I want to know thermocouples location / No of thermocouples vs Pipe size according to API 6A /API 16A for localaised stress relief (PWHT), Any one have the standards let me know or inform where i can get the information.
Thanks
S.Eswaran
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments: