[MW:13890] FW: 13887] welding of SA193 GR B7 Stud ON CS MATERIAL

Use ( 8018-B2  or  7018 ),,, preheat to 150 ,,, PWHT if Thickness >13mm (704 : 706 C ) ( 2.4 Min / mm )

 

Eng. Ahmed Osman

Senior QA/QC Eng.

Orascom Construction Egypt

+20 122 5880434

ahmed.mahmoudmohamed@orascomci.com

a.osman81@yahoo.ca

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of asad azmi
Sent: Wednesday, March 14, 2012 4:18 PM
To: materials-welding@googlegroups.com
Subject: [MW:13887] welding of SA193 GR B7 Stud ON CS MATERIAL

 

Dear All,

 

is it possible to weld SA193 GR B7 Stud on CS material.

 

Please provide name of consumable and preheat/postheat requirement.

 

Thanks & Reagrds

 

Asad Azmi

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...