Hi,
If any material not listed in ASME Sec.IX you should consider as an unassigned material only.
Thanks & Regards,
(Karthik)
Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8, Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Fax : +66 38 897 034
Hand Phone: 0066 892512282
From: Henry Jung <armyamarine@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Wednesday, March 14, 2012 8:42 PM
Subject: [MW:13887] P no to M no
Hi,
As per AWS B2.1, A519 4130 is categorized M No - 11B / Gp No 9.
May I use this no as P & Gp no of ASME code?
This is unlisted in latest ASME Sec. IX.
Thanks & Regards,
Henry
South Korea
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment