Hi.
IN API 570 RECOMENDED 2 LAYER MINIMUN, IN MY EXPERIENCE IQUAL OR MAJOR TO NOMINAL THICKNESS OF HEATHER.
AGUSTIN
De: km hanif <hanif978@gmail.com>
Para: materials-welding@googlegroups.com
Enviado: Sábado, febrero 25, 2012 9:22 A.M.
Asunto: [MW:13784] Weld-O-Let fillet size
Para: materials-welding@googlegroups.com
Enviado: Sábado, febrero 25, 2012 9:22 A.M.
Asunto: [MW:13784] Weld-O-Let fillet size
Dear Experts,
I need your help for the attached subject
We are fabricating some well manifolds as per B31.3, Material ASTM A106. Gr B. header size 4" sch 40 (6.02mm thk) branch connections with 2" sch 80 weld-o-let. How we can calculate the required fillet size and it is required to cover all portion (which area tacking with bore pipe)
Kindly help me,,
I need your help for the attached subject
We are fabricating some well manifolds as per B31.3, Material ASTM A106. Gr B. header size 4" sch 40 (6.02mm thk) branch connections with 2" sch 80 weld-o-let. How we can calculate the required fillet size and it is required to cover all portion (which area tacking with bore pipe)
Kindly help me,,
Thanks & Regards
Hanifa K.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments