Saturday, February 18, 2012

Re: [MW:13729] dished head shape for 2: 1 elleptical dished head

Hi,

if SF is more you are adjusting overal lenghth & template is
suiting there is no problem with dish.

Regards.

Manjunath

On 2/17/12, asad azmi <azmiasadayub@gmail.com> wrote:
> Dear All,
>
> Greetings.
>
> A dished head of ID 1520 mm & thk 80 mm hot formed by subcotractor. A
> vessel is being manufactured by ASME SEC VIII DIV1.
> as per the forming report dished head is having Overcrowning of 10 mm & SF
> is 70 mm.
>
> Now vessel manufacturer is claming that Dished is having 10 mm plus side
> SF( 80 mm). manufacturer wants to shift tan line by 10 mm to maintain
> overall lenght.
>
> my question is --
>
> 1) is it mandatory that for for a dished having overcrowing, SF will
> also be more than required.
>
> 2) what is the effect on Knuckle radius if the SF is shifted by 10mm.(
> considering the fact that contractor has done forming of the dished head
> considering 70 mm SF).
>
> 3) can we accept the dished head if dished head forming contactor certify
> that even with 80MM SF the true shape of the dished head will be
> satisfactory.
>
> *can we accept the dished head if true shape of the dished head is
> checked by a template( 2: 1 elleptical type) which is having 80mm SF & it
> is showing satisfactory result.*
>
> Please advice.
>
> Thanks & Regards
>
> Asad Azmi
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...