RE: [MW:13772] Incomplete pen vide B31.3 2004 Ed

My dear,
IP is in the root, right? In 8" pipe VT is obviously out ruled. My question is, IP being a serious discontinuity, how is it acceptable even for normal fluid service? IQI contrast - indication density, etc is bit untidy, but the main question is not that.
Thanks,
SV

--- On Tue, 21/2/12, vijayan <vijayan.m@madinagulf.com> wrote:

From: vijayan <vijayan.m@madinagulf.com>
Subject: RE: [MW:13767] Incomplete pen vide B31.3 2004 Ed
To: materials-welding@googlegroups.com
Date: Tuesday, 21 February, 2012, 7:00 PM

Hi

 

Ref B31.3

 

The applicable NDT method for this defect is VT and RT.  If it is an open joint check the depth of IP by visual. But in RT you can approximately identify( Not measure) the depth by difference in contrast relative to the IQI contrast at that location

BR

M.Vijayan

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Shashank Vagal
Sent: Tuesday, February 21, 2012 2:12 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:13764] Incomplete pen vide B31.3 2004 Ed

 

Thanks, Manpreet and others,
It was captured during RTFI and the lengths were 12 mm and 25 mm at 2 different locations. I have already given both as repair. But the contractor came with this table which shows Category M fluid, girth weld, weld imperfection ' Incomplete Pen' is referred to as B. On the following page, B refers to "depth" of IP to between ≤1mm and ≤ 0.2Tw (whichever is lower is implied) and not length. Now, that is one tough task to determine depth of an IP, by RT at least. In Cum Length, < 38 mm in 150 mm, we have acceptance.
So, is my judgement correct or no?
Best regards,
Shashank Vagal


--- On Tue, 21/2/12, manpreet <manpreetsin88@rediffmail.com> wrote:


From: manpreet <manpreetsin88@rediffmail.com>
Subject: Re: [MW:13762] Incomplete pen vide B31.3 2004 Ed
To: materials-welding@googlegroups.com
Date: Tuesday, 21 February, 2012, 1:49 PM

Hi,

As per ASME B31.3, acceptance criteria for incomplete penetration is:- between ≤1mm ann ≤0.2Tw

was it caught by Radiography or ultrasonic testing?

If UT then there is possibility that what you are referring to "incomplete penetration" might
actually be "Lack of sidewall fusion" for which table 341.3.2 Note 7 states that
"tightly butted unfused root faces are unacceptable".

Regards
Manpreet Singh



On Tue, 21 Feb 2012 09:11:51 +0530 wrote
>Gents,
REF:
B31.3 Ed 2010, Table 341.3.2
Weld joint of 8" dia x 7 mm thick 106 Gr B, Fluid Service Normal, Category M.
Welding Process: GTAW + SMAW.
Is incomplete pen allowed as per this code to any extent ? Please advise.
Regards,
Shashank Vagal






--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
>

 

Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



This communication and any files transmitted with it are confidential and may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient or the person responsible for delivering it to the intended recipient(s), please note that any form of distribution, copying or use of this communication or information contained in it is strictly prohibited and may be unlawful. If you have received this communication in error please return it to the sender, and delete the material from any computer. We reserve the right to monitor email communications through normal internal and external networks. We believe but not warrant that the email and the attachments are virus free. The statement and opinions expressed in this communication are those of the writer and do not necessarily represent those of Madina Group, whose registered office address is

P.O. Box 20459, Doha, Qatar.
Tel. +974 44600818
Fax. +974 44603143

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...