Re: [MW:13762] How to increase the penetration of P92

change your polarity......

On Tue, Feb 21, 2012 at 4:55 PM, Roy LIU刘艺 <standardliu@hotmail.com> wrote:
>   Dear Experts,
>
>    Recently, I met a problem that there has point defects in the fusion line
> in P92 weld seam.
>    Only UT can find out the defect, but RT can not.
>    When the welder repaired, we find nothing!
>     What are the influence factors?
>     Let's discuss together!
>
>    the pipe is 95mm thick. the electrode is Thermanit MTS 616, 4.0mm.
>    How can I increase the penetration?
>    What is the proper paramete?
>
>
>
>
>    Best regards
>
>
>
>     Roy
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...