Wednesday, February 15, 2012

Re: [MW:13699] Blind thickness design

Hi,

Nobody would be able to answer this unless required information is provided, Which Class,
Material, Size, pressure and temperature...

Please refer ASME B16.5, you will note that Table 22 has maximum size listed as 12" for #2500.
For all other Classes (upto #1500) maximum size is listed as 24".

If your design criteria falls within ASME B16.5 range then Simply Purchase Blind Flange in
accordance with ASME B16.5.

If not then refer ASME Sec Viii Div 1 UG-34 to calculate Blind Flange thickness, Usually it
would not be an easy exercise for a beginner but if you insist, i can send you some
calculations done in my current project (Give me your personnel e-mail ID).

Regards
Manpreet Singh




Dear all,

Can someone help me to calculate the blind
flange thickness for hydrostatic testing.

Thanks and Regards

Anish Dev.S

Gulf East Engg

Qatar









--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
>

Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...