Hi
 
Please specify what grade and thickness of SA517 you are using.
ALso how can your interpass temp. be lesser than your preheat ???
What hardness values you had got in the weld, HAZ and PM during the PQR?
Have you checked the as welded hardness of the consumables E11018M?
 
Regards
 
Prem Nautiyal

--- On Sun, 2/19/12, pradip kumar sil <pradipsil@gmail.com> wrote:

From: pradip kumar sil <pradipsil@gmail.com>
Subject: [MW:13739] How to reduce SA517 hardness
To: materials-welding@googlegroups.com
Cc: "pgoswami" <pgoswami@quickclic.net>
Date: Sunday, February 19, 2012, 2:13 PM

Dear Sir,
We are using one material which is equivalent to SA-517 material (
Pressure  vessel plates, alloy steel, high strength, quenched &
tempered ). with electrode E-11018M. Climatic condition of the
environment is minus 5 degree Centigrade to plus six degree
Centigrade.Parent material hardness is 230 BHN but weld material
hardness is coming approx 400 BHN  which is not acceptable. We are
properly maintaining preheating  i.e 250 degree Centigrade as well as
interpass temperature is 150 degree centigrade.
Pls guide me how can i reduce this material hardness.
Regards
Pradip

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...