Re: [MW:35501] TEST COUPON ASME SEC IX

Yes, You can machine the Plate. 
Prepare the Welding Running Sheet and mention 14 mm Plate machined to 8 mm Plate. 

then the groove weld qualification will be 8-16 mm for impact test and 1.5 - 16 mm without impact test

On Sat, Mar 29, 2025 at 2:58 PM Elavarasan Mech <elavarasan1861994@gmail.com> wrote:
dear sir 
 Actual project thickness :9mm ( impact required)PED
we have 14 mm thick plate SA516 G70 .if considered impact requirement as per ASME SEC IX ( WPS QUALIFICATION )we need minimum base mental thickness  9mm .we plan to weld 14mm plate decrease the thickness to 8mm .still my WPS qualified with impact 8mm To 16 mm.
My consideration is machined plate acceptable or not  which standard I need to refer 


ELAVARASAN


On Sat, 29 Mar 2025 at 10:37 AM Venkatesh Mech <venki2204@gmail.com> wrote:
Hi elavarasan,
Can you elaborate whether you have to machine 14mm plate to 8 mm for welding, or you have to make 8mm plate instead of 14mm. 

Select the weld plate thickness based on your casting weld depth .

Incase your casting weld depth requirement is more than 2 inch better you can for 40mm plate so that you can weld as much as the depth as standard requirement, make sure you have to get approval incase you are doing major weld on the part based on customer requirement.

Regards,
Venkateshwaran 

On Sat, 29 Mar, 2025, 08:30 Elavarasan Mech, <elavarasan1861994@gmail.com> wrote:
Please clarify below 
As per ASME SEC IX can we use 14mm plate machined to 8 mm plate for WPS & WQT qualification.please guide me 
 
Regards 
ELAVARASAN 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ym4-UGqb6tprYjv66ifU7fan--MHmyUneojUPdVkv44Fg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2BY70uaXej5FCPuzr%2BaUD0B0jSPObOYV0E4mkCMj17SDEr0TGg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4y%3D6PGiU6r9LayDvHs%2Bvjin0MpVmWanH_URFvHxBd%2Bd-zQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAGAT7zeEQY00T5kCSKVC8%2BW-ze30e%2BrZ2TCavikPu4F4cDgVUA%40mail.gmail.com.

Saturday, March 29, 2025

Re: [MW:35488] Re: 2411] Re: FW: 2390] Aluminium welding Data

In Aluminium welding, Cleaning Aluminium oxide, hydrated oxide to be cleaned mechanically & by ARC also.  Al2O3 has got melting temperature around 2400 deg celsius whereas Pure aluminium around 660deg celsius. Torch shall be water cooled to avoid high heat inturn, absorb hydrogen which is enemy to form pores. USE AC Square wave with Pure or Zirconiated Tungsten.
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Mar 19, 2025 at 10:25 PM James Bond <jamessbaand.786@gmail.com> wrote:
Dear Sir,

i have a job for aluminimum welding - 3mm sheet + 20 square tube welding.
this is my first time.

can u help me with this. - for aluminum welding.

how to do - how to prepare the surface - gas and welding parameters - pre requisities for aluminium welding.

kind regards,
k. vinodh kumar
hosur, tamil nadu, india
+91-9844035036

On Saturday, June 13, 2009 at 10:08:41 AM UTC+5:30 PB HEGDE wrote:

There is a vast difference in welding practices between Steel and aluminum welding.

i)Commonly Aluminum is welded by Tig and mig process

ii) For Tig process for more than 5mm thk AC tig is preffered with pure argon ,Pure tungsten is used. For AC tig DC suppressor is used for better performance, Preheating .is to be controlled properly. Weld pool is to be well protected from wind. Cleaning of filler metal before use is very essential. In case DC mode use electrode DC +ve to be used

iii)For mig Electrode  DC +ve to be used ,generally 1.2 dia wire on spool is used.

 

iv) For weld properties ,you will not be achieve the UTS as per base material. However 70% of base material strength is acceptable for weld and accordingly the base material thk is designed.

v)Some of the alloy require Aging or Heat treatment to improve the properties.

 

Aluminum welding is not that simple as steel welding as porosity is major problem you will face

 

Regards

 

Hegde P.B.

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of NILESH VARMA
Sent: Friday, June 12, 2009 9:17 AM
To: materials-welding@googlegroups.com
Subject: [MW:2411] Re: FW: 2390] Aluminium welding Data

 

Dear Hegde,
 Firstly thank you for the data given by you. For one of our jobs the material we are using is 6061 T651 as per AMS.
 Actually we wanted to know what are the common differences between steel & aluminium welding & also which are the problems commonly encountered while welding. As our objective is to provide the best product to our customer at low cost we are looking at exploring different fabrication techniques. Also it would obviously we clear to you that since Al is low weight material, the application demands extremely low weight & high strength application.

Regards,
Nilesh V.

On Thu, Jun 11, 2009 at 10:26 AM, PB HEGDE <hegde.pb@isgec.com> wrote:

Dear Nilesh

Attaching the welding and fabrication of aluminum But is there any specific Al alloy in your mind to know

 

Regards

 

Hegde p.B.

 

Subject: FW: 2390] Aluminium welding Data

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of NILESH VARMA
Sent: Wednesday, June 10, 2009 6:26 PM
To: materials-welding@googlegroups.com
Subject: [MW:2390] Aluminium welding Data

 

Dear friends,
 Can anybody help me out to find some really good aluminium welding technical data.

Regards
Nilesh V.

 

 



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/c64fca03-6599-479b-b342-86b985d87a7dn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eP%2BKh9rVhM08MtnxgXFcxnd%3DprBbCbqGmRSaJ6Z-zArcw%40mail.gmail.com.

Re: [MW:35489] Specimen Test location in PQR

You have to refer ASME SEX IX , QW-462 For all desired details

On Thu, Mar 6, 2025 at 12:23 PM kumar sumit <kumarsumities@gmail.com> wrote:
Dear all 
               Can anyone Elaborate test specimens(Tensile, root,face/side bend and toughness test) location in PQR sample  with reference and also Size of specimen in which all test is covered.

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CACCHnjWBosU1CDwrMprBs4AKcs26vsp%2B-pVrnbzsuxDpfj93YA%40mail.gmail.com.


--
Regards,
Rkumar Gohil
7874421813

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CACbJsYLwDr8sdMZSs8%2Bhv7a73VjaeBR20Td6k7ARMxWJ1Lxwhw%40mail.gmail.com.

Re: [MW:35490] Specimen Test location in PQR

Refer ASME Sec.IX  

1. QW-451                                  - Type & no. of tests for PQR
2. QW-462, Fig. 462.1 to 462.3  - Specimen sizes for each tests
3. Fig 463.1(a) to 463.1(d)         - Specimen location

Thanks & Regards

K.Dinesh 



On Thu, Mar 6, 2025 at 10:53 AM kumar sumit <kumarsumities@gmail.com> wrote:
Dear all 
               Can anyone Elaborate test specimens(Tensile, root,face/side bend and toughness test) location in PQR sample  with reference and also Size of specimen in which all test is covered.

Thanks

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CACCHnjWBosU1CDwrMprBs4AKcs26vsp%2B-pVrnbzsuxDpfj93YA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAG5OBYGSXBtXmyXMwok2JF5f3OFCKsUp9O7ZaCofAY0F7Dwk%3DQ%40mail.gmail.com.

Re: [MW:35492] Buttering and overlay

Dear Mr Saini,

 major difference between weld with buttering and weld overlay are given below:
1. weld over lay 
     a. weld over lay have two types, one is hardface over lay another one is corosion resistance over lay 
    b. when we required harder surface with higher hardness than base materail - hardface over lay is being used
    c. when we required corrosion resistant surface in order avoid correcion- corrosion resistance over lay being used 
2. weld with butter 
    a. During dissimilar welding applaiction, buttering being used 
    b, when joining carbon steel to stainless steel, the carbon steel side buttering can be done before joining to SS materail 
    c. purpose of buttering to avoid the dilution effect & lossing of alloying  elements from weld metal 

you can refer AWS welding hand book for your further refernce.
     
 



Regards,
Sankaran.SP
Welding & Metallurgy expert
 


On Thursday 13 March, 2025 at 02:50:03 pm IST, Shahil Saini <sainishahil98@gmail.com> wrote:


Hello All,
Hope all are doing well,

Can anyone please explain the major difference between weld with buttering and weld overlay?

Regards & Thanks,
Shahilkumar Saini



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CALfBO_-cKMu1zr5m9f7nu35uH1%2BcoMdWRsyxqVPiAuqKKeay2Q%40mail.gmail.com.

[MW:35494]

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eO2M9p-UQvRRdaBYEgphck%3DTpSB71ygRombbawL-NLpbQ%40mail.gmail.com.

[MW:35496] TEST COUPON ASME SEC IX

Please clarify below 
As per ASME SEC IX can we use 14mm plate machined to 8 mm plate for WPS & WQT qualification.please guide me 
 
Regards 
ELAVARASAN 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ym4-UGqb6tprYjv66ifU7fan--MHmyUneojUPdVkv44Fg%40mail.gmail.com.

Re: [MW:35495] Re: welding of cladded (alloy 625) pipes with single side access


Hi
Thanks for this wonderful insight,even CS bullets on groove for fitup can cause cracking.
Any suggestions on how-to carry out fit up in such scenario.
Thanks in Advance


On Thu, 13 Mar, 2025, 12:54 HUY HOÀNG, <taotengiang000@gmail.com> wrote:
dear sirs,
Cant use 7018 right after ernicrmo-3 finish. You must have butter in between, otherwise it will cause cracking. Thats for sure. We havent even mentioned the heating issue yet.

Vào lúc 13:18:21 UTC+7 ngày Thứ Tư, 8 tháng 6, 2016, Jithesh Premachandran đã viết:
Hi Nikdin,

After buttering (around 1.5mm thick alloy 625 overlay), machine it and match both ID. Then weld the root and hot pass with GTAW (ERNiCrMo-3) then fill up passes with SMAW process. 
Dont deposit any carbon steel deposits on the groove. Even you use Carbon steel bullets for fit up will leads to crack of groove weld deposits.


On Tuesday, May 24, 2016 at 1:40:39 PM UTC+4, Himan Nikdin wrote:
Dear Experts

I need a practical guide or sample WPS for welding of cladded (alloy 625) carbon steel pipes with one side access. the size of pipes are minimum  4".

Regards,
H.Nikdin

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/81a025a1-2968-40bc-9dee-8c0c2dd68eb4n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAMDG82BOnS%3DBNwLxp-G0GoYOjRu_ABs_1gOyJUfdMOctVE7L6w%40mail.gmail.com.

Re: [MW:35497] TEST COUPON ASME SEC IX

Hi elavarasan,
Can you elaborate whether you have to machine 14mm plate to 8 mm for welding, or you have to make 8mm plate instead of 14mm. 

Select the weld plate thickness based on your casting weld depth .

Incase your casting weld depth requirement is more than 2 inch better you can for 40mm plate so that you can weld as much as the depth as standard requirement, make sure you have to get approval incase you are doing major weld on the part based on customer requirement.

Regards,
Venkateshwaran 

On Sat, 29 Mar, 2025, 08:30 Elavarasan Mech, <elavarasan1861994@gmail.com> wrote:
Please clarify below 
As per ASME SEC IX can we use 14mm plate machined to 8 mm plate for WPS & WQT qualification.please guide me 
 
Regards 
ELAVARASAN 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ym4-UGqb6tprYjv66ifU7fan--MHmyUneojUPdVkv44Fg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2BY70uaXej5FCPuzr%2BaUD0B0jSPObOYV0E4mkCMj17SDEr0TGg%40mail.gmail.com.

Re: [MW:35498] TEST COUPON ASME SEC IX

Yes we can use. Write in as Run sheet 16mm plate machined to 8 mm.

On Sat, 29 Mar 2025, 8:30 am Elavarasan Mech, <elavarasan1861994@gmail.com> wrote:
Please clarify below 
As per ASME SEC IX can we use 14mm plate machined to 8 mm plate for WPS & WQT qualification.please guide me 
 
Regards 
ELAVARASAN 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ym4-UGqb6tprYjv66ifU7fan--MHmyUneojUPdVkv44Fg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEabyKnxUeBK3ihVAwyXRasjZfKDKmV%3Dhw0Lx3770JCCTFmEMA%40mail.gmail.com.

Re: [MW:35498] TEST COUPON ASME SEC IX

Wps 
As per my opinion, If qualified 8mm plate min 5mm and Max 2T, weld metal -2t.


On Sat, 29 Mar, 2025, 08:30 Elavarasan Mech, <elavarasan1861994@gmail.com> wrote:
Please clarify below 
As per ASME SEC IX can we use 14mm plate machined to 8 mm plate for WPS & WQT qualification.please guide me 
 
Regards 
ELAVARASAN 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ym4-UGqb6tprYjv66ifU7fan--MHmyUneojUPdVkv44Fg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CABHGzEUreiX52fSUOKQoBekWdsxiYmtsDq_hwEoW8UfJ15h6aw%40mail.gmail.com.

Re: [MW:35500] TEST COUPON ASME SEC IX

dear sir 
 Actual project thickness :9mm ( impact required)PED
we have 14 mm thick plate SA516 G70 .if considered impact requirement as per ASME SEC IX ( WPS QUALIFICATION )we need minimum base mental thickness  9mm .we plan to weld 14mm plate decrease the thickness to 8mm .still my WPS qualified with impact 8mm To 16 mm.
My consideration is machined plate acceptable or not  which standard I need to refer 


ELAVARASAN


On Sat, 29 Mar 2025 at 10:37 AM Venkatesh Mech <venki2204@gmail.com> wrote:
Hi elavarasan,
Can you elaborate whether you have to machine 14mm plate to 8 mm for welding, or you have to make 8mm plate instead of 14mm. 

Select the weld plate thickness based on your casting weld depth .

Incase your casting weld depth requirement is more than 2 inch better you can for 40mm plate so that you can weld as much as the depth as standard requirement, make sure you have to get approval incase you are doing major weld on the part based on customer requirement.

Regards,
Venkateshwaran 

On Sat, 29 Mar, 2025, 08:30 Elavarasan Mech, <elavarasan1861994@gmail.com> wrote:
Please clarify below 
As per ASME SEC IX can we use 14mm plate machined to 8 mm plate for WPS & WQT qualification.please guide me 
 
Regards 
ELAVARASAN 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ym4-UGqb6tprYjv66ifU7fan--MHmyUneojUPdVkv44Fg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2BY70uaXej5FCPuzr%2BaUD0B0jSPObOYV0E4mkCMj17SDEr0TGg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4y%3D6PGiU6r9LayDvHs%2Bvjin0MpVmWanH_URFvHxBd%2Bd-zQ%40mail.gmail.com.

Thursday, March 20, 2025

[MW:35485] Aluminium welding

Dear Sirs,

i need technical details on aluminium welding.

could anyone help me with aluminium welding.

kind regards,
K Vinodh kumar
Hosur, tamilnadu
+91-9844035036

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEwToa_B_Hp4kX7U%2BxKeFdx0FKYFh8aY6urzjsxWytrZ9%3DJ3NQ%40mail.gmail.com.

[MW:35485] Re: 2411] Re: FW: 2390] Aluminium welding Data

Dear Sir,

i have a job for aluminimum welding - 3mm sheet + 20 square tube welding.
this is my first time.

can u help me with this. - for aluminum welding.

how to do - how to prepare the surface - gas and welding parameters - pre requisities for aluminium welding.

kind regards,
k. vinodh kumar
hosur, tamil nadu, india
+91-9844035036

On Saturday, June 13, 2009 at 10:08:41 AM UTC+5:30 PB HEGDE wrote:

There is a vast difference in welding practices between Steel and aluminum welding.

i)Commonly Aluminum is welded by Tig and mig process

ii) For Tig process for more than 5mm thk AC tig is preffered with pure argon ,Pure tungsten is used. For AC tig DC suppressor is used for better performance, Preheating .is to be controlled properly. Weld pool is to be well protected from wind. Cleaning of filler metal before use is very essential. In case DC mode use electrode DC +ve to be used

iii)For mig Electrode  DC +ve to be used ,generally 1.2 dia wire on spool is used.

 

iv) For weld properties ,you will not be achieve the UTS as per base material. However 70% of base material strength is acceptable for weld and accordingly the base material thk is designed.

v)Some of the alloy require Aging or Heat treatment to improve the properties.

 

Aluminum welding is not that simple as steel welding as porosity is major problem you will face

 

Regards

 

Hegde P.B.

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of NILESH VARMA
Sent: Friday, June 12, 2009 9:17 AM
To: materials-welding@googlegroups.com
Subject: [MW:2411] Re: FW: 2390] Aluminium welding Data

 

Dear Hegde,
 Firstly thank you for the data given by you. For one of our jobs the material we are using is 6061 T651 as per AMS.
 Actually we wanted to know what are the common differences between steel & aluminium welding & also which are the problems commonly encountered while welding. As our objective is to provide the best product to our customer at low cost we are looking at exploring different fabrication techniques. Also it would obviously we clear to you that since Al is low weight material, the application demands extremely low weight & high strength application.

Regards,
Nilesh V.

On Thu, Jun 11, 2009 at 10:26 AM, PB HEGDE <hegde.pb@isgec.com> wrote:

Dear Nilesh

Attaching the welding and fabrication of aluminum But is there any specific Al alloy in your mind to know

 

Regards

 

Hegde p.B.

 

Subject: FW: 2390] Aluminium welding Data

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of NILESH VARMA
Sent: Wednesday, June 10, 2009 6:26 PM
To: materials-welding@googlegroups.com
Subject: [MW:2390] Aluminium welding Data

 

Dear friends,
 Can anybody help me out to find some really good aluminium welding technical data.

Regards
Nilesh V.

 

 



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/c64fca03-6599-479b-b342-86b985d87a7dn%40googlegroups.com.

Re: [MW:35487] Aluminium welding

Dear SIr,

Please refer to the following link hereafter:


Best regards,


Le mer. 19 mar. 2025 à 16:55, James Bond <jamessbaand.786@gmail.com> a écrit :
Dear Sirs,

i need technical details on aluminium welding.

could anyone help me with aluminium welding.

kind regards,
K Vinodh kumar
Hosur, tamilnadu
+91-9844035036

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEwToa_B_Hp4kX7U%2BxKeFdx0FKYFh8aY6urzjsxWytrZ9%3DJ3NQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CANRRH0Ldu81ne02i4dcP_5mmhjx9-dYJp%3DnFW_ZB3TdWu7nhog%40mail.gmail.com.

Thursday, March 13, 2025

Re: [MW:35477] WPS for Furnace PWHT

The spools have 1" to 36" Piping joints.
The WPS with PWHT is available only for large diameter / high thickness.
can we do PWHT in the furnace if small size piping joints welded without PWHT WPS which is welding with higher size spools require PWHT?.



On Mon, 27 Jan 2025 at 11:50, Vishwas Keskar <vvkeskar123@gmail.com> wrote:
Pl elaborate your query 
Query is not clear 
Sent from my iPhone

On 27 Jan 2025, at 11:57 AM, Prakash Kumar Bontra <prakashbontra@gmail.com> wrote:


For furnace PWHT as per ASME B 31.3 all the joints in the spool (1" to 36") need PWHT approved WPS and where to refer?

Prakash Bontra

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CANeLWoNy0URXS9X7TEvvZRVe4V-1LNPKwidHJ097fDyPAjyh7Q%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/9C99E29D-02AE-4D96-87E5-8B83DEE92269%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAAR7VZ-G6sd_svwhNprPev55zdMMLPP-GM%3DVKCXFFCrrk%2BCaUw%40mail.gmail.com.

Re: [MW:35479] Welding of CS+Alloy825 clad pipies

HI SIR
I use E309 or E310 for buttering layers. Is it correct ?
I use ernicrmo-3 for root, hot, f1, f2 
then i use E309 in 2 layers
Completely with k7018 to the end. 
It can or can not do it?
Thank you for answering me.
Hope u have a great day

Vào lúc 00:44:35 UTC+7 ngày Chủ Nhật, 11 tháng 7, 2010, pgoswami đã viết:
Hi Romiomdabre,
 
The default technique for such pipe spool (where welding from I/S is not possible) would be to use Inconel-625(E/ER-NiCrMo-3) fillers and electrodes all through. Yes this would make  cost of welding quite high. As you know these piping are exposed for extremely harsh service environments, proven welding consumables are required to meet the design and construction and service requirements. Typical offshore pipeline design specifications such as DNV-OS-F-101 indicates one "type" of welding consumable for single sides welding of clad pipes.
 
I would think there are  some alternatives practiced in the industry,  in the way of using Stainless/ Nickel Based alloys for clad welding + application a pure Iron barrier layer on the clad weld followed by welding with C.S electrodes on C.S base metal. The attached extract of 10064-Page2(15) Fig-26 shows the welding sequences. While this technique has been proven for welding of S.S clad C.S pipes, there had not been much information available on the same for welding of Inconel Clad pipes. The critical factors here is the availability of Pure Iron electrode and acceptance of the same by fabrication code. A sample from Lincoln Electric is attached for information.If any other forum members could shed some lights on this issue,it would be appreciated.
 
Incidentally similar query was raised in another forum,few years ago.I have attached the responses and discussions for
 
Thanks
 
Pradip Goswami,P.Eng.
Welding & Metallurgical Engineer/Specialist
Ontario Power Generation Inc.
Email-pgoswami@sympatico.ca,
 


From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of B.Vaithiyanathan
Sent: Thursday, July 08, 2010 11:14 AM
To: materials-welding
Subject: Re: [MW:5904] Welding of CS+Alloy825 clad pipies

Hi 
       The Consumable for your case is ER NiCrMo3/E NiCrMo3

Regards,
Vaithiyanathan

On Thu, Jul 8, 2010 at 2:52 PM, romio dabre <romio...@gmail.com> wrote:
Dear All
 
We have to weld 20" to 36" pipe spools with following details. Joints cannot be backwelded or cannot do clad restoration from inside.
Material CS+Alloy 825 clad
Thk between 20mm to 54mm
Complete weld with Alloy 625 will be very costly as the thk is high.
What will be the recommended welding consumable combination.
 
Thnaks
 

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With Best Regards

B.Vaithiyanathan

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/c8dd9575-7444-4541-bc34-abe1c8efaec2n%40googlegroups.com.

[MW:35481] Re: welding of cladded (alloy 625) pipes with single side access

dear sirs,
Cant use 7018 right after ernicrmo-3 finish. You must have butter in between, otherwise it will cause cracking. Thats for sure. We havent even mentioned the heating issue yet.

Vào lúc 13:18:21 UTC+7 ngày Thứ Tư, 8 tháng 6, 2016, Jithesh Premachandran đã viết:
Hi Nikdin,

After buttering (around 1.5mm thick alloy 625 overlay), machine it and match both ID. Then weld the root and hot pass with GTAW (ERNiCrMo-3) then fill up passes with SMAW process. 
Dont deposit any carbon steel deposits on the groove. Even you use Carbon steel bullets for fit up will leads to crack of groove weld deposits.


On Tuesday, May 24, 2016 at 1:40:39 PM UTC+4, Himan Nikdin wrote:
Dear Experts

I need a practical guide or sample WPS for welding of cladded (alloy 625) carbon steel pipes with one side access. the size of pipes are minimum  4".

Regards,
H.Nikdin

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/81a025a1-2968-40bc-9dee-8c0c2dd68eb4n%40googlegroups.com.

[MW:35482] Buttering and overlay

Hello All,
Hope all are doing well,

Can anyone please explain the major difference between weld with buttering and weld overlay?

Regards & Thanks,
Shahilkumar Saini



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CALfBO_-cKMu1zr5m9f7nu35uH1%2BcoMdWRsyxqVPiAuqKKeay2Q%40mail.gmail.com.

Re: [MW:35483] Pipe Insert Sleeve - How to ensure after hydrotest No Water

Hi

The black 'O' Ring seals the gap between pipe and sleeve, 

Also a TK epoxy system "blue mastic" is applied all over the sleeve except weld area,

 After all this there will be no water entry during hydro test in the weld joint area, 

regards,
Sreeraj

On Tue, Nov 12, 2024 at 2:09 PM 'SENTHILKUMAR SWAMINATHAN' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Mr. Aravindh,

Thank you for your reply.
How did you have ensured there is no water between sleeve insert and pipe?
This insert used not to get corrosion inside weld joint area. While performing trail we have prove that no hydrotested water entered in very tiny gap. 

Thank you, 
Regards, 
S.SENTHILKUMAR


On Tuesday 12 November, 2024 at 05:47:07 am GMT+3, s.aravindh ram <aravindhram22@gmail.com> wrote:


Dear sir,
I have worked in oman,  used this  high pressure line we will apply gloves insert this bevel joint after welding welding complete hydrotest will be conducted as per designed pressure,
After that testing we will the spool for erection.
Thankyou
Aravindh


On Fri, 8 Nov 2024, 7:09 pm 'SENTHILKUMAR SWAMINATHAN' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Dear All,

Please see below picture Pipe Insert Sleeve in my site taking trial and completed hydrotest as proto type. Now how to ensure there is no water between Pipeline and insert sleeve. 
Any body have experienced in this please give feedback. 
Thanks 
Inline image


Thank you, 
Regards, 
S.SENTHILKUMAR

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/115108384.237400.1731070617477%40mail.yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAGH_84AoxZnJcJez4FnCTxduc984PsFksajgiq6kmHPVen2wTg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/2062804084.1072071.1731405752365%40mail.yahoo.com.


--
Thanks & Regards,

Sreeraj. V
+968 97807131
+91 9895752398

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAMzX%3DQgAgw0WHDkO-saFicPtta5cEUdTm3xyxDC5-PSJoGKAaA%40mail.gmail.com.

Saturday, March 8, 2025

[MW:35448] Hot tapping between piping and pipeline

Dear Expert
we have hot tapping 
from process piping b31.3 design 
to cross country pipeline old pipe i think api 1104 design
WPS that need to folow  api 1104 or asme b31.3.
best regard.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/ffa0c881-23d8-4b3f-96d1-7337ed4ac1e1n%40googlegroups.com.

Re: [MW:35449] Hot tapping between piping and pipeline

Hi

You have to follow API 1104 Annex B for qualifying the procedure

Regards
Hrishikesan

On Mon, Feb 24, 2025 at 8:24 AM ali owead <aliawead1@gmail.com> wrote:
Dear Expert
we have hot tapping 
from process piping b31.3 design 
to cross country pipeline old pipe i think api 1104 design
WPS that need to folow  api 1104 or asme b31.3.
best regard.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/ffa0c881-23d8-4b3f-96d1-7337ed4ac1e1n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAFHBd_8d%2BLmRBsV9kM6vdJHaSJ1%2BRmZO8C_45V%3D%3DOQ%3DusRqbjA%40mail.gmail.com.

[MW:35450] WPS PQR STELLITE 6 HARD FACING ON WC9

Hi experts 

Does anyone have WPS pqr for stellite-6 Hardfacing weld overlay on A217 WC9 base material . Please share with me

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADazMagmqFQbCnf0W_sVoNMxn5_F5CQi8WbAMsWB4Ta02O0Urw%40mail.gmail.com.

[MW:35451] Piping Butt weld joint resting on support

Hy,
   Good day. Can any expert give me a reference for Piping joint can't  rest of Pipe Support or any part of structure?? Is there any International standard cover this topic ??

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/434d282d-2951-4d30-bab7-94c92e45bb51n%40googlegroups.com.

Re: [MW:35452] Piping Butt weld joint resting on support

As per international standards:

ASME B31.3 (Clause 321.1.2, 321.1.3) – Piping joints should not rest on supports to prevent undue stress and allow inspection.

ASME B31.1 (Clause 114.3, 120.1) – Supports must not interfere with expansion or place stress on joints.

API 570 – Ensures accessibility for inspection and maintenance.

MSS SP-58 – Recommends support placement away from joints.

Regards
Deerendra


On Tue, 25 Feb, 2025, 21:09 Mudssar Raza, <mudassar.raza7867@gmail.com> wrote:
Hy,
   Good day. Can any expert give me a reference for Piping joint can't  rest of Pipe Support or any part of structure?? Is there any International standard cover this topic ??

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/434d282d-2951-4d30-bab7-94c92e45bb51n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAG0nF9E3VjH6TysU_BL3V2cxm7sG07JMC0CYWgxu5M_1Jho_Dg%40mail.gmail.com.

[MW:35453] WELDER PERFORMANCE RECORD

Dear Experts,

Does anyone have welder performance record format. If so, could you kindly share it with me. I would like to use it to monitor welder performance and present the data to the client.

BR,
Midhun

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/a82f2a5e-2341-4544-8d1f-68b65e65503dn%40googlegroups.com.

Re: [MW:35454] WELDER PERFORMANCE RECORD



‫في الأربعاء، 26 فبراير 2025 في 11:45 ص تمت كتابة ما يلي بواسطة ‪Midhun murali‬‏ <‪muralimidhun15@gmail.com‬‏>:‬
Dear Experts,

Does anyone have welder performance record format. If so, could you kindly share it with me. I would like to use it to monitor welder performance and present the data to the client.

BR,
Midhun

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/a82f2a5e-2341-4544-8d1f-68b65e65503dn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAB0C2x_d2XAxQU1UAKSk-eL4u10WfVrLk63k6kQ68Ej3KP8zTw%40mail.gmail.com.

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...