Wednesday, September 30, 2020

[MW:31528] distance between corrosion probe& coupon

Dear All.
Does any body know which standard or even specification of oil and gas company said about minimum Longitudinal distance of corrosion probe and corrosion coupon?
Regards.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/7c263a5d-1891-4532-8322-256e85082b91n%40googlegroups.com.

Re: [MW:31526] ASME Material Re-certification

Dear,

Q.Few Plates & Pipes have few remaining marking.  
A. You should ask your perchaser for MTC from vendor.
and secound option. mail to concerned directly for MTC . 
the vendor may be give you MTC if you provide the detail of plate or pipe.


On Sat, Sep 26, 2020 at 11:50 PM hardik desai <hvdesai1284@gmail.com> wrote:
Hello Sir,
               I have few Plates & Pipes which are in the open yard (Open to atmosphere condition) since last 10 years. Few Plates & Pipes have few remaining marking. MTCs are also not available. Shall we re-certify and use it after 10 years? 

              Is there any Provisions for Max.validity of Material Certification by Code, If i even retrieve all MTCs somehow for the materials which are still having marking on it? 

Regards,
Hardik Desai  

On Sun, Sep 27, 2020 at 11:09 AM George Dilintas <dilintas@gmail.com> wrote:
You have to explain to the inspector that the physics of the metallurgy dont make any difference between plates and pipes. This is basic metallurgy

Στις Παρ, 25 Σεπ 2020 στις 1:58 μ.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Thank you George for the precise information. However, whether the inspector accept SA-20(for plates) when we perform above mentioned activities on seamless pipes like SA-106, although the chemical elements are similar on pipes and plates.

Kind Regards

On Fri, 25 Sep 2020, 3:20 pm George Dilintas, <dilintas@gmail.com> wrote:
The answer is given in SA-20 - 8.3.2. If your Al content is 0,020% or higher you dont need to do any test

Στις Παρ, 25 Σεπ 2020 στις 7:13 π.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Thank you George for your valuable advice. If you see PG 10.2.2.3, it requires the documentation of killed steel. How to document whether the steel is killed or not, except mentioning the Silicon/Aluminium content. Is it possible to perform some tests?

Best Regards

On Wed, 23 Sep 2020 at 17:20, George Dilintas <dilintas@gmail.com> wrote:
Since the Code is Sect I + B31.1 you have to use PG-10. The  approach is similar to UG-10.  Since you lack full identification  and If you know the spec of the materials then you implement PG-10.2 . If not then you implement PG-10.3. In both cases you have to perform chemical analysis and mechanical tests

Στις Τρί, 22 Σεπ 2020 στις 10:17 π.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Dears,
         How can I recertify raw pipes, where the material certificates are missing/cannot be recovered..! The code of construction is ASME Sec I & B31.1. As per Sec viii UG-10, is it possible to recertify pipes that don't have certificates, by performing mechanical tests? Please share your knowledge with regard to this. Your reply would be highly appreciated.

Best Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc27-ctAGkf6NwMnbsOdAfZug65Xg4pK8ADLAmKMw22QG8iA%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bbjsu2vzKooYW5bOX--xCWfCJ_sn-FDSXc8RBseZbAOw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc279aQd_ix0metsDVAWirnkxuqhH2A3OmFhNYuVDQXDYb_Q%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bc8KN3uoL%2B6KzXBxtnrVqUe7zfCNOe1EGUmM_e%2B5e88g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc279Agtfr-%3D8DPG5OJ-xsSY3PeLsjJp2FsuRr%2B%2B7SKFm_-g%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bx2qNgj5PVzM79RMGzsA47JVLTGAi%3D9CEDMz2XDb6rBw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADbW%2BUu8B-bXn%2B8APqkg%2BNOB%2B4qeiDzpnPtfH3OSwjcOuKOnGg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHnLYC%2B_eQfJ3abaxEor7Wi%2BTjjA_WWqjeUohRd9c7ktHV%3D-aw%40mail.gmail.com.

Tuesday, September 29, 2020

Re: [MW:31527] ASME Material Re-certification

1. I suppose you need to examine the conditions of Plate and Pipe before it is being used.
2. Plate and Pipe may be subjected to Atmospheric corrosion and observed with Pits. So you need to check whether the minimum thickness Tolerance as given in SA-20 for Plates & Sa-530 for Pipes is complied.
3, MTC is not an issue, if Traceability is Available then you can check with the Mill/stockist for MTC else you can create an identification and do the tests as recommended by Material standard.
4. 10 years is quite a long period, no restriction in code some clients like Tatweer Bahrain put restriction on Year of manufacturing to 5 years and hence check the specification.

Thanks & Regards

J.Gerald Jayakumar




On Tuesday, 29 September, 2020, 04:32:23 pm GMT+7, GMT <gmt.lah@gmail.com> wrote:


Dear,

Q.Few Plates & Pipes have few remaining marking.  
A. You should ask your perchaser for MTC from vendor.
and secound option. mail to concerned directly for MTC . 
the vendor may be give you MTC if you provide the detail of plate or pipe.


On Sat, Sep 26, 2020 at 11:50 PM hardik desai <hvdesai1284@gmail.com> wrote:
Hello Sir,
               I have few Plates & Pipes which are in the open yard (Open to atmosphere condition) since last 10 years. Few Plates & Pipes have few remaining marking. MTCs are also not available. Shall we re-certify and use it after 10 years? 

              Is there any Provisions for Max.validity of Material Certification by Code, If i even retrieve all MTCs somehow for the materials which are still having marking on it? 

Regards,
Hardik Desai  

On Sun, Sep 27, 2020 at 11:09 AM George Dilintas <dilintas@gmail.com> wrote:
You have to explain to the inspector that the physics of the metallurgy dont make any difference between plates and pipes. This is basic metallurgy

Στις Παρ, 25 Σεπ 2020 στις 1:58 μ.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Thank you George for the precise information. However, whether the inspector accept SA-20(for plates) when we perform above mentioned activities on seamless pipes like SA-106, although the chemical elements are similar on pipes and plates.

Kind Regards

On Fri, 25 Sep 2020, 3:20 pm George Dilintas, <dilintas@gmail.com> wrote:
The answer is given in SA-20 - 8.3.2. If your Al content is 0,020% or higher you dont need to do any test

Στις Παρ, 25 Σεπ 2020 στις 7:13 π.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Thank you George for your valuable advice. If you see PG 10.2.2.3, it requires the documentation of killed steel. How to document whether the steel is killed or not, except mentioning the Silicon/Aluminium content. Is it possible to perform some tests?

Best Regards

On Wed, 23 Sep 2020 at 17:20, George Dilintas <dilintas@gmail.com> wrote:
Since the Code is Sect I + B31.1 you have to use PG-10. The  approach is similar to UG-10.  Since you lack full identification  and If you know the spec of the materials then you implement PG-10.2 . If not then you implement PG-10.3. In both cases you have to perform chemical analysis and mechanical tests

Στις Τρί, 22 Σεπ 2020 στις 10:17 π.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Dears,
         How can I recertify raw pipes, where the material certificates are missing/cannot be recovered..! The code of construction is ASME Sec I & B31.1. As per Sec viii UG-10, is it possible to recertify pipes that don't have certificates, by performing mechanical tests? Please share your knowledge with regard to this. Your reply would be highly appreciated.

Best Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc27-ctAGkf6NwMnbsOdAfZug65Xg4pK8ADLAmKMw22QG8iA%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bbjsu2vzKooYW5bOX--xCWfCJ_sn-FDSXc8RBseZbAOw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc279aQd_ix0metsDVAWirnkxuqhH2A3OmFhNYuVDQXDYb_Q%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bc8KN3uoL%2B6KzXBxtnrVqUe7zfCNOe1EGUmM_e%2B5e88g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc279Agtfr-%3D8DPG5OJ-xsSY3PeLsjJp2FsuRr%2B%2B7SKFm_-g%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bx2qNgj5PVzM79RMGzsA47JVLTGAi%3D9CEDMz2XDb6rBw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADbW%2BUu8B-bXn%2B8APqkg%2BNOB%2B4qeiDzpnPtfH3OSwjcOuKOnGg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHnLYC%2B_eQfJ3abaxEor7Wi%2BTjjA_WWqjeUohRd9c7ktHV%3D-aw%40mail.gmail.com.

Sunday, September 27, 2020

Re: [MW:31525] ASME Material Re-certification

Try ASME Sec-IIA   SA-530.

Thanks & Regards

J.Gerald Jayakumar



On Sunday, 27 September, 2020, 06:22:25 pm GMT+7, Sourav Bohrays <souravbohrays@gmail.com> wrote:


sa20 and sa106 are different spec diff manufacturing process how you can comply on basis of other spec this is unacceptable recertify only basis of related specification

On Sun, 27 Sep 2020, 11:52 am Sourav Bohrays, <souravbohrays@gmail.com> wrote:
for this case firstly raise NCR than go for mechanical n chemical testing than recertify to specification nd edition you required.

On Sun, 27 Sep 2020, 10:50 am hardik desai, <hvdesai1284@gmail.com> wrote:
Hello Sir,
               I have few Plates & Pipes which are in the open yard (Open to atmosphere condition) since last 10 years. Few Plates & Pipes have few remaining marking. MTCs are also not available. Shall we re-certify and use it after 10 years? 

              Is there any Provisions for Max.validity of Material Certification by Code, If i even retrieve all MTCs somehow for the materials which are still having marking on it? 

Regards,
Hardik Desai  

On Sun, Sep 27, 2020 at 11:09 AM George Dilintas <dilintas@gmail.com> wrote:
You have to explain to the inspector that the physics of the metallurgy dont make any difference between plates and pipes. This is basic metallurgy

Στις Παρ, 25 Σεπ 2020 στις 1:58 μ.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Thank you George for the precise information. However, whether the inspector accept SA-20(for plates) when we perform above mentioned activities on seamless pipes like SA-106, although the chemical elements are similar on pipes and plates.

Kind Regards

On Fri, 25 Sep 2020, 3:20 pm George Dilintas, <dilintas@gmail.com> wrote:
The answer is given in SA-20 - 8.3.2. If your Al content is 0,020% or higher you dont need to do any test

Στις Παρ, 25 Σεπ 2020 στις 7:13 π.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Thank you George for your valuable advice. If you see PG 10.2.2.3, it requires the documentation of killed steel. How to document whether the steel is killed or not, except mentioning the Silicon/Aluminium content. Is it possible to perform some tests?

Best Regards

On Wed, 23 Sep 2020 at 17:20, George Dilintas <dilintas@gmail.com> wrote:
Since the Code is Sect I + B31.1 you have to use PG-10. The  approach is similar to UG-10.  Since you lack full identification  and If you know the spec of the materials then you implement PG-10.2 . If not then you implement PG-10.3. In both cases you have to perform chemical analysis and mechanical tests

Στις Τρί, 22 Σεπ 2020 στις 10:17 π.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Dears,
         How can I recertify raw pipes, where the material certificates are missing/cannot be recovered..! The code of construction is ASME Sec I & B31.1. As per Sec viii UG-10, is it possible to recertify pipes that don't have certificates, by performing mechanical tests? Please share your knowledge with regard to this. Your reply would be highly appreciated.

Best Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc27-ctAGkf6NwMnbsOdAfZug65Xg4pK8ADLAmKMw22QG8iA%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bbjsu2vzKooYW5bOX--xCWfCJ_sn-FDSXc8RBseZbAOw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc279aQd_ix0metsDVAWirnkxuqhH2A3OmFhNYuVDQXDYb_Q%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bc8KN3uoL%2B6KzXBxtnrVqUe7zfCNOe1EGUmM_e%2B5e88g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc279Agtfr-%3D8DPG5OJ-xsSY3PeLsjJp2FsuRr%2B%2B7SKFm_-g%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bx2qNgj5PVzM79RMGzsA47JVLTGAi%3D9CEDMz2XDb6rBw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADbW%2BUu8B-bXn%2B8APqkg%2BNOB%2B4qeiDzpnPtfH3OSwjcOuKOnGg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAOWr6k_iBGoRgTAifYbk33KuzdeLD1uaFRbar6PyW0ZaEiCaEw%40mail.gmail.com
.

Re: [MW:31523] ASME Material Re-certification

sa20 and sa106 are different spec diff manufacturing process how you can comply on basis of other spec this is unacceptable recertify only basis of related specification

On Sun, 27 Sep 2020, 11:52 am Sourav Bohrays, <souravbohrays@gmail.com> wrote:
for this case firstly raise NCR than go for mechanical n chemical testing than recertify to specification nd edition you required.

On Sun, 27 Sep 2020, 10:50 am hardik desai, <hvdesai1284@gmail.com> wrote:
Hello Sir,
               I have few Plates & Pipes which are in the open yard (Open to atmosphere condition) since last 10 years. Few Plates & Pipes have few remaining marking. MTCs are also not available. Shall we re-certify and use it after 10 years? 

              Is there any Provisions for Max.validity of Material Certification by Code, If i even retrieve all MTCs somehow for the materials which are still having marking on it? 

Regards,
Hardik Desai  

On Sun, Sep 27, 2020 at 11:09 AM George Dilintas <dilintas@gmail.com> wrote:
You have to explain to the inspector that the physics of the metallurgy dont make any difference between plates and pipes. This is basic metallurgy

Στις Παρ, 25 Σεπ 2020 στις 1:58 μ.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Thank you George for the precise information. However, whether the inspector accept SA-20(for plates) when we perform above mentioned activities on seamless pipes like SA-106, although the chemical elements are similar on pipes and plates.

Kind Regards

On Fri, 25 Sep 2020, 3:20 pm George Dilintas, <dilintas@gmail.com> wrote:
The answer is given in SA-20 - 8.3.2. If your Al content is 0,020% or higher you dont need to do any test

Στις Παρ, 25 Σεπ 2020 στις 7:13 π.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Thank you George for your valuable advice. If you see PG 10.2.2.3, it requires the documentation of killed steel. How to document whether the steel is killed or not, except mentioning the Silicon/Aluminium content. Is it possible to perform some tests?

Best Regards

On Wed, 23 Sep 2020 at 17:20, George Dilintas <dilintas@gmail.com> wrote:
Since the Code is Sect I + B31.1 you have to use PG-10. The  approach is similar to UG-10.  Since you lack full identification  and If you know the spec of the materials then you implement PG-10.2 . If not then you implement PG-10.3. In both cases you have to perform chemical analysis and mechanical tests

Στις Τρί, 22 Σεπ 2020 στις 10:17 π.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Dears,
         How can I recertify raw pipes, where the material certificates are missing/cannot be recovered..! The code of construction is ASME Sec I & B31.1. As per Sec viii UG-10, is it possible to recertify pipes that don't have certificates, by performing mechanical tests? Please share your knowledge with regard to this. Your reply would be highly appreciated.

Best Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc27-ctAGkf6NwMnbsOdAfZug65Xg4pK8ADLAmKMw22QG8iA%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bbjsu2vzKooYW5bOX--xCWfCJ_sn-FDSXc8RBseZbAOw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc279aQd_ix0metsDVAWirnkxuqhH2A3OmFhNYuVDQXDYb_Q%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bc8KN3uoL%2B6KzXBxtnrVqUe7zfCNOe1EGUmM_e%2B5e88g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc279Agtfr-%3D8DPG5OJ-xsSY3PeLsjJp2FsuRr%2B%2B7SKFm_-g%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bx2qNgj5PVzM79RMGzsA47JVLTGAi%3D9CEDMz2XDb6rBw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADbW%2BUu8B-bXn%2B8APqkg%2BNOB%2B4qeiDzpnPtfH3OSwjcOuKOnGg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWr6k_iBGoRgTAifYbk33KuzdeLD1uaFRbar6PyW0ZaEiCaEw%40mail.gmail.com.

Re: [MW:31523] ASME Material Re-certification

for this case firstly raise NCR than go for mechanical n chemical testing than recertify to specification nd edition you required.

On Sun, 27 Sep 2020, 10:50 am hardik desai, <hvdesai1284@gmail.com> wrote:
Hello Sir,
               I have few Plates & Pipes which are in the open yard (Open to atmosphere condition) since last 10 years. Few Plates & Pipes have few remaining marking. MTCs are also not available. Shall we re-certify and use it after 10 years? 

              Is there any Provisions for Max.validity of Material Certification by Code, If i even retrieve all MTCs somehow for the materials which are still having marking on it? 

Regards,
Hardik Desai  

On Sun, Sep 27, 2020 at 11:09 AM George Dilintas <dilintas@gmail.com> wrote:
You have to explain to the inspector that the physics of the metallurgy dont make any difference between plates and pipes. This is basic metallurgy

Στις Παρ, 25 Σεπ 2020 στις 1:58 μ.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Thank you George for the precise information. However, whether the inspector accept SA-20(for plates) when we perform above mentioned activities on seamless pipes like SA-106, although the chemical elements are similar on pipes and plates.

Kind Regards

On Fri, 25 Sep 2020, 3:20 pm George Dilintas, <dilintas@gmail.com> wrote:
The answer is given in SA-20 - 8.3.2. If your Al content is 0,020% or higher you dont need to do any test

Στις Παρ, 25 Σεπ 2020 στις 7:13 π.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Thank you George for your valuable advice. If you see PG 10.2.2.3, it requires the documentation of killed steel. How to document whether the steel is killed or not, except mentioning the Silicon/Aluminium content. Is it possible to perform some tests?

Best Regards

On Wed, 23 Sep 2020 at 17:20, George Dilintas <dilintas@gmail.com> wrote:
Since the Code is Sect I + B31.1 you have to use PG-10. The  approach is similar to UG-10.  Since you lack full identification  and If you know the spec of the materials then you implement PG-10.2 . If not then you implement PG-10.3. In both cases you have to perform chemical analysis and mechanical tests

Στις Τρί, 22 Σεπ 2020 στις 10:17 π.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Dears,
         How can I recertify raw pipes, where the material certificates are missing/cannot be recovered..! The code of construction is ASME Sec I & B31.1. As per Sec viii UG-10, is it possible to recertify pipes that don't have certificates, by performing mechanical tests? Please share your knowledge with regard to this. Your reply would be highly appreciated.

Best Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc27-ctAGkf6NwMnbsOdAfZug65Xg4pK8ADLAmKMw22QG8iA%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bbjsu2vzKooYW5bOX--xCWfCJ_sn-FDSXc8RBseZbAOw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc279aQd_ix0metsDVAWirnkxuqhH2A3OmFhNYuVDQXDYb_Q%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bc8KN3uoL%2B6KzXBxtnrVqUe7zfCNOe1EGUmM_e%2B5e88g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc279Agtfr-%3D8DPG5OJ-xsSY3PeLsjJp2FsuRr%2B%2B7SKFm_-g%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bx2qNgj5PVzM79RMGzsA47JVLTGAi%3D9CEDMz2XDb6rBw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADbW%2BUu8B-bXn%2B8APqkg%2BNOB%2B4qeiDzpnPtfH3OSwjcOuKOnGg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOWr6k8dzc3Fr1igA%3DHXe_HxPYfHm23v7EKrCEe5hRLJFLAS%2BQ%40mail.gmail.com.

Re: [MW:31522] ASME Material Re-certification

Hello Sir,
               I have few Plates & Pipes which are in the open yard (Open to atmosphere condition) since last 10 years. Few Plates & Pipes have few remaining marking. MTCs are also not available. Shall we re-certify and use it after 10 years? 

              Is there any Provisions for Max.validity of Material Certification by Code, If i even retrieve all MTCs somehow for the materials which are still having marking on it? 

Regards,
Hardik Desai  

On Sun, Sep 27, 2020 at 11:09 AM George Dilintas <dilintas@gmail.com> wrote:
You have to explain to the inspector that the physics of the metallurgy dont make any difference between plates and pipes. This is basic metallurgy

Στις Παρ, 25 Σεπ 2020 στις 1:58 μ.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Thank you George for the precise information. However, whether the inspector accept SA-20(for plates) when we perform above mentioned activities on seamless pipes like SA-106, although the chemical elements are similar on pipes and plates.

Kind Regards

On Fri, 25 Sep 2020, 3:20 pm George Dilintas, <dilintas@gmail.com> wrote:
The answer is given in SA-20 - 8.3.2. If your Al content is 0,020% or higher you dont need to do any test

Στις Παρ, 25 Σεπ 2020 στις 7:13 π.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Thank you George for your valuable advice. If you see PG 10.2.2.3, it requires the documentation of killed steel. How to document whether the steel is killed or not, except mentioning the Silicon/Aluminium content. Is it possible to perform some tests?

Best Regards

On Wed, 23 Sep 2020 at 17:20, George Dilintas <dilintas@gmail.com> wrote:
Since the Code is Sect I + B31.1 you have to use PG-10. The  approach is similar to UG-10.  Since you lack full identification  and If you know the spec of the materials then you implement PG-10.2 . If not then you implement PG-10.3. In both cases you have to perform chemical analysis and mechanical tests

Στις Τρί, 22 Σεπ 2020 στις 10:17 π.μ., ο/η Rejoy Thomas <rejoythomas90@gmail.com> έγραψε:
Dears,
         How can I recertify raw pipes, where the material certificates are missing/cannot be recovered..! The code of construction is ASME Sec I & B31.1. As per Sec viii UG-10, is it possible to recertify pipes that don't have certificates, by performing mechanical tests? Please share your knowledge with regard to this. Your reply would be highly appreciated.

Best Regards

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc27-ctAGkf6NwMnbsOdAfZug65Xg4pK8ADLAmKMw22QG8iA%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bbjsu2vzKooYW5bOX--xCWfCJ_sn-FDSXc8RBseZbAOw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc279aQd_ix0metsDVAWirnkxuqhH2A3OmFhNYuVDQXDYb_Q%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bc8KN3uoL%2B6KzXBxtnrVqUe7zfCNOe1EGUmM_e%2B5e88g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALLc279Agtfr-%3D8DPG5OJ-xsSY3PeLsjJp2FsuRr%2B%2B7SKFm_-g%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40Bx2qNgj5PVzM79RMGzsA47JVLTGAi%3D9CEDMz2XDb6rBw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADbW%2BUu8B-bXn%2B8APqkg%2BNOB%2B4qeiDzpnPtfH3OSwjcOuKOnGg%40mail.gmail.com.

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs