Sunday, July 31, 2016
Re: [MW:25175] how to calculate hydrostatic head
P=pressure
q= densiry of water 1000kg/m3
g= 9.81m/s2
H=head suppose 10 m
P= 98100N/m2
P=1.013kg/cm2
Where 1 N= 1 kg.m/s2
Hence @ 10 m height we consider pressure 1 kg/cm2.
Regards
Kunal Patel
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/66fc2fae-3bec-44f4-adef-43d27ac30aad%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:25174] Multiple welders can weld in a single production joint?
Dear Mr.Jijilal,
The pdf attachment is production weld mockups for Procedure and performance qualification.
The production weld is the first joint which a welder welds after the qualification of his welder qualification test specimen.
Regards,
Hareesh K V
Please refer the attachment--Best Regards,JIJILAL K.M.QA/QC Manager,Thai Jurong Engineering Ltd,KCE SPP Project,Thailand#096 786 0129On 29 July 2016 at 17:11, Rajakani A <araja192@gmail.com> wrote:--Dear friends,Can multiple welders weld in a single production joint in same process and position?Kindly clarify me with reference ASME standards if any.Regards,Rajakani A,L&T Construction,Surat.+91-7874201744.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4733b8e2-5b61-4e6d-9838-6baa0baadd77%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHiUTkbai5CSKpgXNicHLU8w4dsMo2TFqxj4_R2E0u7vzA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM3LgAUdvVVYeK6qQ2SOEJsoLWjUhmCEPpkNgYifP_d8DvxEAQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:25173] RE: 24605] 3/4" Tube weld RT
You can use x rays with slow film for.better result.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4fb26d98-e3e6-4548-aca0-89d5915665ab%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHAXWsMwn84125_JnkyZHrkP_7FC2iaes%2BmGFW0yPTooUmcDkQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
RE: [MW:25171] Multiple welders can weld in a single production joint?
Alan Denney
AKD Materials Consulting Ltd
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Hareesh K V
Sent: 30 July 2016 17:08
To: materials-welding@googlegroups.com
Subject: Re: [MW:25169] Multiple welders can weld in a single production joint?
Dear friend,
This can be done as there is no code restrictions. If the joint is failed all the welders are considered to be failed.
For bigger diameter pipes say, 60" which is usually welded by more than one welder this can be accepted.
The concept of the production weld is to understand the ability of the welder in a real job situation. So on that basis try to avoid using multiple welders in one production joint.
Regards,
Hareesh K V
Sent from my Samsung Galaxy smartphone.
-------- Original message --------
From: Rajakani A <araja192@gmail.com>
Date: 29/07/2016 3:41 p.m. (GMT+05:30)
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:25157] Multiple welders can weld in a single production joint?
Dear friends,
Can multiple welders weld in a single production joint in same process and position?
Kindly clarify me with reference ASME standards if any.
Regards,
Rajakani A,
L&T Construction,
Surat.
+91-7874201744.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4733b8e2-5b61-4e6d-9838-6baa0baadd77%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/dldxs1hjoqq88m8dlohuim6f.1469894902247%40email.android.com.
For more options, visit https://groups.google.com/d/optout.
Saturday, July 30, 2016
Re: [MW:25170] Multiple welders can weld in a single production joint?
From: Rajakani A Sent: Σάββατο, 30 Ιουλίου 2016 - 09:38 To: Materials & Welding Reply To: materials-welding@googlegroups.com Subject: [MW:25157] Multiple welders can weld in a single production joint? |
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4733b8e2-5b61-4e6d-9838-6baa0baadd77%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:25169] Multiple welders can weld in a single production joint?
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4733b8e2-5b61-4e6d-9838-6baa0baadd77%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:25168] RF pad clashing with circumferential pipe weld joints
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHjWb9xPp0KfV_gBBZh2Xu3Cm33QVuu8TjPAVW_SFmBUsA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:25167] Multiple welders can weld in a single production joint?
--Dear friends,Can multiple welders weld in a single production joint in same process and position?Kindly clarify me with reference ASME standards if any.Regards,Rajakani A,L&T Construction,Surat.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4733b8e2-5b61-4e6d-9838-6baa0baadd77%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOenW4i9dDNQsUe1%2B9YyvMyYsv4TaEMkUDLERT7dBz8ROFmD1Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:25171] Multiple welders can weld in a single production joint?
--Dear friends,Can multiple welders weld in a single production joint in same process and position?Kindly clarify me with reference ASME standards if any.Regards,Rajakani A,L&T Construction,Surat.+91-7874201744.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4733b8e2-5b61-4e6d-9838-6baa0baadd77%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHiUTkbai5CSKpgXNicHLU8w4dsMo2TFqxj4_R2E0u7vzA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:25166] Re: Tack welder qualification
Be sure that tack welders dont open arc out if bevel.
Date: Thu, 28 Jul 2016 21:05:20 +0300
Subject: Re: [MW:25156] Re: Tack welder qualification
From: dilintas@gmail.com
To: materials-welding@googlegroups.com
...if they remain in place...Sent from my BlackBerry 10 smartphone.
From: anthony chundalSent: Πέμπτη, 28 Ιουλίου 2016 - 13:04To: Materials & WeldingReply To: materials-welding@googlegroups.comSubject: [MW:25155] Re: Tack welder qualificationDear Sam,As per ASME Sec VIII-Div-1, UW-31(c), tack welders need to be qualified.Regards,Anthony.
On Tuesday, December 13, 2011 at 8:48:37 PM UTC+4, samshuddin k wrote:Dear Experts
There is any clause in ASME Sec. IX for tack welder qualification.
Which Code explains tack welder qualification for piping
regards
Samshuddin.K
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cc0d08ba-e64a-49a5-9402-5354a48c9a48%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160728180520.6713423.18949.3894%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BLU183-W15A51C161BD8FC45EFA3828F010%40phx.gbl.--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHggn7m8YPraKd08aZ-M3aeuLvV5EwVn0LVmLBnhzE0p5w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:25165] RF pad clashing with circumferential pipe weld joints
--Dear Experts,Refer to subject line and attachment , An RF pad is coming closely with the circumferential weld of a lateral Tee.Please advice how to resolve it. Code is ASME B 31.1.Best Regards,JIJILAL K.M.Thai Jurong Engineering Ltd,KCE SPP Project,Thailand
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHjWb9xPp0KfV_gBBZh2Xu3Cm33QVuu8TjPAVW_SFmBUsA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNKBVJ8KEBvZ7VR3jQUvWWKtD95Tj%2B%2Bm_10f8DTQVMF3A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:25163] Full form of SFA
Dear Expert,
Please help me regarding below full form,
SFA 5.1 (aws classification of carbon steel electrode).....what does mean of SFA????
Regards,
Raneesh.ok
--
Sr.Qc engineer-kochi refinery
Cswip 3.1 & ASNT
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGRQ%2BmX-pFVRpFAYcvBmrSW%2Bv3n3z4fq2sctdDEuJvfv2aFwog%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHj%3D_ko_dy-zLzKO6C71BfQw%3DxQK8KEyXAE6q4pgQ5WMWA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
[MW:25163] RF pad clashing with circumferential pipe weld joints
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHjWb9xPp0KfV_gBBZh2Xu3Cm33QVuu8TjPAVW_SFmBUsA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:25162] Full form of SFA
Dear Expert,
Please help me regarding below full form,
SFA 5.1 (aws classification of carbon steel electrode).....what does mean of SFA????
Regards,
Raneesh.ok
--
Sr.Qc engineer-kochi refinery
Cswip 3.1 & ASNT
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGRQ%2BmX-pFVRpFAYcvBmrSW%2Bv3n3z4fq2sctdDEuJvfv2aFwog%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8kNjpPs%3DYfsEZTzWERyunusBpLwsqVAx8idv-K5ObfXvg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:25161] Full form of SFA
Dear Expert,
Please help me regarding below full form,
SFA 5.1 (aws classification of carbon steel electrode).....what does mean of SFA????
Regards,
Raneesh.ok
--
Sr.Qc engineer-kochi refinery
Cswip 3.1 & ASNT
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGRQ%2BmX-pFVRpFAYcvBmrSW%2Bv3n3z4fq2sctdDEuJvfv2aFwog%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACdTRdwMpeHR0LxQVmLY9X42an_JfGwbymMJ_CAQjZ0x8rsDcQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:25160] PWHT
This information is gold, few people know.Regards!.To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5Zur%2BjbHf849DKFr%2BA_H6Ye2BsercDSdxh3H0w4id8C35xMA%40mail.gmail.com.--2016-07-27 1:49 GMT-05:00 Krisanu Bhunia <krisanu.bunty@gmail.com>:thank you, A537 CL1 is P1 marital but which thickness can do welding and which clause it is mention--On Tue, Jul 26, 2016 at 8:45 PM, José Juan Jiménez Alejandro <jjjimeneza@gmail.com> wrote:BPVC ASME Section VIII Div 1, allows welding after the PWHT, but only for materials P1 and P3 and only certain thickness, but remember that this code is only for new equipment, not for equipment being repaired, if this is your building code ahead !.--2016-07-25 3:41 GMT-05:00 ishwar kumar <ish8623@gmail.com>:--Dear sir,In clean out door in tank we found welding not sufficient after PWHT.(A 537 CL1)SO, now need to welding again . PWHT again doing or can avoid it by which code ?Regardskrisanu bhunia
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMZth3qmH8a3w0Efd96-M12HsymvR61YRPz18j1nOFpdZME9PQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4797E08A-DC0C-48F2-924D-5F0F5CA2C326%40gmail.com.--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--Ing. Jose Juan Jimenez Alejandro
Cel. 8116171750
Skype: jjjimeneza
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/uHRzkNOaGNw/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurK%3DsL48-4rGdYMqNxnQNa7ZKXYkqoiE7rMePC7mpAu48w%40mail.gmail.com.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMZth3r9R93LbPOOBr%2B1cQVttdywdCK36QHp3Upjh%2B2SRrt4yQ%40mail.gmail.com.--Ing. Jose Juan Jimenez Alejandro
Cel. 8116171750
Skype: jjjimeneza
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9cd%3DtVmBffbRD_s4wtstSL0va-vVDKohtNDAGR5B2Ec%3Dg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
[MW:25157] Full form of SFA
Dear Expert,
Please help me regarding below full form,
SFA 5.1 (aws classification of carbon steel electrode).....what does mean of SFA????
Regards,
Raneesh.ok
Sr.Qc engineer-kochi refinery
Cswip 3.1 & ASNT
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGRQ%2BmX-pFVRpFAYcvBmrSW%2Bv3n3z4fq2sctdDEuJvfv2aFwog%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Friday, July 29, 2016
RE: [MW:25157] Re: Tack welder qualification
Date: Thu, 28 Jul 2016 21:05:20 +0300
Subject: Re: [MW:25156] Re: Tack welder qualification
From: dilintas@gmail.com
To: materials-welding@googlegroups.com
From: anthony chundal Sent: Πέμπτη, 28 Ιουλίου 2016 - 13:04 To: Materials & Welding Reply To: materials-welding@googlegroups.com Subject: [MW:25155] Re: Tack welder qualification |
On Tuesday, December 13, 2011 at 8:48:37 PM UTC+4, samshuddin k wrote:
Dear Experts
There is any clause in ASME Sec. IX for tack welder qualification.
Which Code explains tack welder qualification for piping
regards
Samshuddin.K
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cc0d08ba-e64a-49a5-9402-5354a48c9a48%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160728180520.6713423.18949.3894%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
[MW:25157] Multiple welders can weld in a single production joint?
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4733b8e2-5b61-4e6d-9838-6baa0baadd77%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Thursday, July 28, 2016
Re: [MW:25156] Re: Tack welder qualification
From: anthony chundal Sent: Πέμπτη, 28 Ιουλίου 2016 - 13:04 To: Materials & Welding Reply To: materials-welding@googlegroups.com Subject: [MW:25155] Re: Tack welder qualification |
On Tuesday, December 13, 2011 at 8:48:37 PM UTC+4, samshuddin k wrote:
Dear Experts
There is any clause in ASME Sec. IX for tack welder qualification.
Which Code explains tack welder qualification for piping
regards
Samshuddin.K
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cc0d08ba-e64a-49a5-9402-5354a48c9a48%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Re: [MW:25154] use of PN16 flanges dimensions are as per EN 1092-1 for asme div-1
From: Hemant W Joshi Sent: Πέμπτη, 28 Ιουλίου 2016 - 08:51 To: materials-welding@googlegroups.com Reply To: materials-welding@googlegroups.com Subject: RE: [MW:25152] use of PN16 flanges dimensions are as per EN 1092-1 for asme div-1 |
What is the type of flange, size in question?
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of anthony chundal
Sent: Wednesday, July 27, 2016 7:07 PM
To: Materials & Welding
Subject: [MW:25151] use of PN16 flanges dimensions are as per EN 1092-1 for asme div-1
Please advice whether we can use PN16 flanges dimensions are as per EN 1092-1 without providing any calculations as per appendix -2, for ASME Div-1 pressure vessel, material specification is SA105,
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6a44a704-4339-4191-a555-1ff396a4ab96%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
----------------------------------------------------------------------------------------------------------
Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately.
Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences.
While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail.
---------------------------------------------------------------------------------------------------------
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c8097cf1b9fb4aa3b4f647bc8abd542c%40MUMEXG02.TCE.COM.
For more options, visit https://groups.google.com/d/optout.
[MW:35725] Dismillar material Welding
Dear experts, In my Hydro Electric Project materials using A517Gr.F and A537CL-II. For A517Gr.F using E 11018M and A537CL-II using E 9018...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...