Re: [MW:13701] Can we do tack weld by pipe fitters?

Dear all,

The question is " Can we do tack weld by pipe fitters according to ASME 31.3? "

so, we should go to ASME B31.3.

The Code said on part 328.5.1 (c) Tack welds shall be made by a qualified welder or welding operator.

Regards,
Doni Afrizal
IdWI, ASNT NDT Level 2 (MT,PT,RI)

On Wed, Feb 15, 2012 at 6:19 PM, manpreet <manpreetsin88@rediffmail.com> wrote:
Hi,

Qualification is required (see applicable design code).

e.g. ASME VIII/1, UW-31 CUTTING, FITTING, AND ALIGNMENT
….
(c) …..Tack welds, whether removed or left in place, shall be made using a fillet weld or butt
weld procedure qualified in accordance with Section IX. …

Regards
Manpreet Singh




On Wed, 15 Feb 2012 09:04:56 +0530 wrote

>Can we do tack weld by pipe fitters according to ASME 31.3?



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...