Tuesday, February 21, 2012

Re: [MW:13762] Incomplete pen vide B31.3 2004 Ed

Hi,

As per ASME B31.3, acceptance criteria for incomplete penetration is:- between ≤1mm ann ≤0.2Tw

was it caught by Radiography or ultrasonic testing?

If UT then there is possibility that what you are referring to "incomplete penetration" might
actually be "Lack of sidewall fusion" for which table 341.3.2 Note 7 states that
"tightly butted unfused root faces are unacceptable".

Regards
Manpreet Singh



On Tue, 21 Feb 2012 09:11:51 +0530 wrote
>Gents,
REF:
B31.3 Ed 2010, Table 341.3.2
Weld joint of 8" dia x 7 mm thick 106 Gr B, Fluid Service Normal, Category M.
Welding Process: GTAW + SMAW.
Is incomplete pen allowed as per this code to any extent ? Please advise.
Regards,
Shashank Vagal






--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
>
Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...