As per my opinion..they want to take avg of thickness for defined grid size rather taking a spot measurement..
Logic behind must be a limitation of mfgg to give uniform thickness throught the cross section in complete length..but this will be in benifit to u..

On Feb 22, 2012 12:45 PM, "khatri ankit" <nids01dme011@gmail.com> wrote:
Dear Experts,

In NPCIL project specification for seamless Alloy steel
fittings,following sentence will be given as

- Minimum thk will be calculated on grid size minimum 30mm for up to
50NB & 50mm for up to   500NB & 100mm for above size.

I never heard about this,

I want some information regarding this matter.

Kindly share ur thoughts about this topic and give some referances

regards,

Ankit Khatri

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35725] Dismillar material Welding

Dear experts,  In my Hydro Electric Project  materials using A517Gr.F and A537CL-II.  For A517Gr.F using E 11018M and A537CL-II using E 9018...