Dear Anil Kumar You an use ENiCu7 or ERNiCu7 for welding monel to SS Regards Hegde P.B.
--- On Mon, 20/2/12, jaya anil <nethalaanil@gmail.com> wrote:
From: jaya anil <nethalaanil@gmail.com> Subject: [MW:13750] Re: welding of Monel (P40) E.Tee to SS Pipe(304) To: materials-welding@googlegroups.com Date: Monday, 20 February, 2012, 1:13 PM
Dear Experts, Please let me know the Electrode or filler rod to be used to Qualify a WPS for Monel(P40) to SS(P8) .I have to qulify a procedure for welding this both at site. regards Anil Kumar -- To post to this group, send email to materials-welding@googlegroups.comTo unsubscribe from this group, send email to materials-welding+ unsubscribe@googlegroups.comFor more options, visit this group's bolg at http://materials-welding.blogspot.com/The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments