Saturday, February 18, 2012

Re: [MW:13737] For expiration of welders for WPQ

Dear Mr.Ankit,

Upon satisfactory performance of the welder you can renew his qualification for every six month without re-qualification. But if the welder has the gap of more than six month in welding or any question arises on his performance, then the welder should be requalified to demonstrate his skills and ability.
 
 
With Regards,
s.sundarrajan,
QA/QC Inspector,
Special technical services LLC, Muscat,
M: +96898217243.


From: khatri ankit <nids01dme011@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Friday, 17 February 2012 3:59 PM
Subject: [MW:13725] For expiration of welders for WPQ

Dear Experts,

I have confusion about validity for the welder qualification.

As per ASME Sec-IX, QW-322, When welder has not welded withe process
during the period of 6 months or more his qualification for that
process shall expire unless within 6 months period prior to his
expiration of qualification.

i have doubt that if welder is doing welding for particular process
since 1 yr under my supervision, the will i need some renewal?

shall the welder expired or not within 6 months period if he is doing
welding for particular process:

Kindly justify this clause


Regards,

Ankit Khatri

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...