On Feb 25, 8:52 pm, km hanif <hanif...@gmail.com> wrote:
> Dear Experts,
> I need your help for the attached subject
>
> We are fabricating some well manifolds as per B31.3, Material ASTM A106. Gr
> B. header size 4" sch 40 (6.02mm thk) branch connections with 2" sch 80
> weld-o-let. How we can calculate the required fillet size and it is
> required to cover all portion (which area tacking with bore pipe)
>
> Kindly help me,,
>
> Thanks & Regards
>
> Hanifa K.
>
> Weld O let.bmp
> 1552KViewDownload
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments