Saturday, February 18, 2012

Re: [MW:13733] For expiration of welders for WPQ

You can renew it with record proof within the 6 months period where RT or UT accepted on his weld.
 
Regards,
S.SENTHILKUMAR
From: Feroz Mohammed <feroz.bv@gmail.com>
To: materials-welding@googlegroups.com
Sent: Saturday, 18 February 2012 6:48 AM
Subject: Re: [MW:13728] For expiration of welders for WPQ

You may requalify him or may continue as him, also depends on customer & contractor mutual agreement.

On Fri, Feb 17, 2012 at 5:29 PM, khatri ankit <nids01dme011@gmail.com> wrote:
Dear Experts,

I have confusion about validity for the welder qualification.

As per ASME Sec-IX, QW-322, When welder has not welded withe process
during the period of 6 months or more his qualification for that
process shall expire unless within 6 months period prior to his
expiration of qualification.

i have doubt that if welder is doing welding for particular process
since 1 yr under my supervision, the will i need some renewal?

shall the welder expired or not within 6 months period if he is doing
welding for particular process:

Kindly justify this clause


Regards,

Ankit Khatri

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards
Feroz Mohammed
Deputy Manager-QA&I
LANCO Infratech Ltd.
È : +91 9650490097
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...