Dear Mr.Krishna Kumar,

Branch weld is possible using suitable fittings like weldolet or T, provided you have access for applying the kniffing filler at the branch portion.
Branch pipe is possible until 4" size for cement lined, below which the piping shall be provided with suitable internal lining for protection of the piping.

Regards,

Murthy.J.N 

On Mon, Feb 13, 2012 at 12:22 PM, Krishnakumar M S <krishnakumarms01@yahoo.com> wrote:
Dear Experts,

I want to tap 6" line from 10" header which is internally cement lined. Pipe configurations are

MOC                : A106 Gr.B
Service               : Sea Water
Pressure            :   5 kg/sq.cm

Please tell me if branch weld is possible..!! , what is the minimum size possible for branch line (for Branch weld).

Regards,
 
KRISHNAKUMAR.M.S
Piping Engineer
Fact Engineering & Design Organization (FEDO)
KERALA, INDIA

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...