Monday, February 20, 2012

Re: [MW:13748] Incomplete pen vide B31.3 2004 Ed

Depth of Incomplete Penetration allowed  : 1mm and less
Cumulative Length                                     : 38mm and less in any 150mm weld length
 
Thanks & Regards

J.Gerald Jayakumar0091-9344954677
From: Shashank Vagal <nach_sam@yahoo.com>
To: materials-welding@googlegroups.com
Cc: peymanhafezi@gmail.com
Sent: Sunday, February 19, 2012 1:38 PM
Subject: [MW:13739] Incomplete pen vide B31.3 2004 Ed
Gents,
REF:
B31.3 Ed 2010, Table 341.3.2
Weld joint of 8" dia x 7 mm thick 106 Gr B, Fluid Service Normal, Category M.
Welding Process: GTAW + SMAW.
Is incomplete pen allowed as per this code to any extent ? Please advise.
Regards,
Shashank Vagal


-- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/ The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...