Hi,

Please describe your application?

Test is more applicable for Pipelines where there is possibility that in an event of small
crack, it might run through quite a distance.

API5L Table18 & ASME B31.8 requires DWTT for linepipe after reaching a certain diameter
(If agreed, DWT testing of Pipe Body of welded pipe with D>508mm = Once per test unit of pipe)

Result values are specified in Percentage shear (ASTM E436), It assures resistance to ductility
running fracture if shear is 85% or better at the min. design temp. of the line, which a charly
bar does not, Test Coupon is comparably bigger than Charpy testing.


Regards
Manpreet Singh





From: Mohit Aggarwal
[mailto:aggarwalmohit05@gmail.com]
>Sent: Tuesday, February 14, 2012
10:17 AM
>To: materials-welding
>Cc:
christopher_rajku...@yahoo.com; george.dilintas@gr.bureauveritas.com;
manojac...@gmail.com; welding_engr_r...@charter.net; AA karandish; Abuhanip bin
Abdul; Ahmed Osman; akcme; Ali Asghari; Aly; AMIT PAHUJA; Amos Majola; Anil
Hegde; antony jenis; Arun Jacob; Arunachalam A; Ary Agung Prasetyo; asad azmi;
Brl Pp; Dindo; Dinesh Somwanshi; duc hoang; ENAYAT ZAREI; Endri Prasetyo; Fitria
Rahman; fredric; Garry Mat Eng.; Himan Nikdin; james gerald; John Henning; jose;
Kaja Mohideen; kannayeram gnanapandithan; Karthik; Kavin Murugam; ketan shah;
khemici badri; lakshman kumar; Madhusudan Rout; mahesh sanghvi; Mahmoud; meemo
prasad; Mehdi Emami; mpk mpk; MRG; Muhammed Ibrahim PK; muthu barathi; Nadgauda,
Subhas; Nandesh Kumar; Narendra Gohil; Neilash Kumar; Nizam Mohamad; pgoswami;
Pieper QSI; prabhakarmet@gmail.com; prem nautiyal; R.Lenin; rajeev arora;
rajkumarantoni; Ramchandra vichare; Ramin Kondori; ravi varman; S C Balawat;
sanggyu LEE; santhosh kumar; SAQIB SHIRAZI; sevak hiren; Shadab Alam Ansari;
shanmuga mari; snbagchi; Srinivas Engr; srinivasu; T. Mahendran; U WYNN-NAING;
vaibhav Joshi; venkat ramana; Vijay Katkar; vinit.deshpande; Vino Varghese; Wu
Hua; yogeshkumar Kumbhar; ZUL MAS
>Subject: Drop Weight
Test.
>
>
Respected Experts,

>
As per client Requirement We will have to conduct Drop Weight Test IN
NPCIL.. What is Drop Weight Test and how we will determine Nil ductility
transition temp..PLease reply

>
Thanks & REgards
MOhit Aggarwal.



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
>

Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...