Monday, February 27, 2012

Re: [MW:13787] Ferrite Number.....

This change in ferrite content is probably due to cooling rate difference .... related to solidification process.

Prashant Nimbalkar


From: shanmugam govindarajan <rajansgr@yahoo.com>
To: MW-Google Groups. <materials-welding@googlegroups.com>
Sent: Saturday, February 25, 2012 5:16 AM
Subject: [MW:13777] Ferrite Number.....

Dear Experts,
 
During Ferrite check on the strip cladding, we noticed FN as 1.5, 2, 2.5 whereas project specn requires 3 to 10.
These low FN is noticed near the cirseam joints in the vessel. May be the first or last pass of strip cladding when strip cladding is done in each shell. 
Please send me some info about root cause, remedial action that is to be taken and reference to code/specn. 
 
With regards,
Govi.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...