Dear
This is only Good engineering Practice. You can perform MPI if there is any reason to doubt
for crack development. Otherwise it should not be cut.
Anyway final NDT is going to be performed.
There no such code requirement and I strongly recommend not to cut the same.

P.K.Mishra
Ahmedabad, India

On Fri, 17 Feb 2012 10:46:13 +0530 wrote
>Dear experts,





I need your help, In our project (B.31.3) CS pipe joints ASTM A106 Gr.B 8" Sch XXS, our
construction team kept the joints after root pass and hot pass welding, but our QC instructed
to cut and and re-weld the joints. Really it is required and it is mentioned any were in code?
We are maintaining preheat at 150-Deg and inter pass temp 300-Deg
Please help me;;;;

>
>



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.
>

Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35725] Dismillar material Welding

Dear experts,  In my Hydro Electric Project  materials using A517Gr.F and A537CL-II.  For A517Gr.F using E 11018M and A537CL-II using E 9018...