Re: [MW:13791] Details about lateral expansion in impact testing.

Dear, trichy

Please refer UHA-51 of ASME SECOND VIII DIV - 1.

Regards,
Chirag Patel.

Sent from BlackBerry® on Airtel

-----Original Message-----
From: "g.venkatesan06@gmail.com" <g.venkatesan06@gmail.com>
Sender: materials-welding@googlegroups.com
Date: Tue, 28 Feb 2012 03:24:17
To: materials-welding@googlegroups.com<materials-welding@googlegroups.com>
Reply-To: materials-welding@googlegroups.com
Subject: [MW:13790] Details about lateral expansion in impact testing.

Dear experts, iam freshers in fabrication field. Can any one give me the answers for the following question. 1. What is lateral expansion. 2. Why it is required instead of J in impact testing. 3. What is the acceptable value of lateral expansion in stainless steel and carbon and low alloy steel. Show the code reference our code of construction is ASME Sec VIII Div1. Regards venkat/sisco projects, trichy

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...