Hi !
To get good Impact properties in SS weld you should
i) Flux should be of basic nature having bsisity bet 3-3.5
ii)Interpass should be max 150C
iii) No preheating for SS
iv) Adjust current Voltage and SAw speed to get bead height not more than 2.5mm
Try to cool the weld as fast as possible
Regards
Hegde P.B.

--- On Fri, 24/2/12, pawan <pawan.tiwari@dwekam.org> wrote:

From: pawan <pawan.tiwari@dwekam.org>
Subject: [MW:13776] SS welding with SAW
To: materials-welding@googlegroups.com
Date: Friday, 24 February, 2012, 4:37 PM

Dear Experts,
Could anyone suggest me about the followings for stainless steel SAW welding to reach >0.38mm %LE at -196deg. cen.

 

  1. Limitation of wire composition for ER308L grade wire.
  2. SAW welding parameters. (A/V/Speed)
  3. Preheating & Heat input for more than 50mm thick plate.
  4. Any other special requirement.

 

Rgd

Pawan Tiwari

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...