Wednesday, February 15, 2012

Re: [MW:13700] Can we do tack weld by pipe fitters?

Hi,

Qualification is required (see applicable design code).

e.g. ASME VIII/1, UW-31 CUTTING, FITTING, AND ALIGNMENT
….
(c) …..Tack welds, whether removed or left in place, shall be made using a fillet weld or butt
weld procedure qualified in accordance with Section IX. …

Regards
Manpreet Singh




On Wed, 15 Feb 2012 09:04:56 +0530 wrote
>Can we do tack weld by pipe fitters according to ASME 31.3?



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for
educational purposes only, Users must take their own decisions w.r.t. applicable
code/standard/contract documents.


Follow Rediff Deal ho jaye! to get exciting offers in your city everyday.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35763] Hardness range for CS+ Alloy0625 clad welding

Dear experts. I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. Both material consists of a base metal with alloy...